EN 1465 Adhesives Lap Shear Bond Strength of Rigid-to-Rigid Assemblies
Written by Meredith Bernstein
- Adhesives
- Tension
- EN 1465
EN 1465 is a tensile test used to measure the adhesive lap-shear bond strength of rigid-to-rigid assemblies. This standard is used by many industries to test adhesives applied to materials such as metals, plastics, wood, and composites. Lap-shear strength is a critical characteristic of any adhesive, as they can exhibit unique shear properties.
EN 1465 is extremely similar to ISO 4587 with the exception of test rate. Both standards use identical test setups, specimen geometries, and results reporting, with the exception that ISO 4587 calls out a specific test rate of 8.3MPa to 9.8MPa while EN 1465 only specifies a constant rate of load application. Both standards state that the average specimen should break in a period of 65+/-20 sec.
Materials Testing SystemEN1465 is performed on a universal testing machine with a system capacity dependent on the strength of the adhesive. Most tests to this standard will fall into the capacity range between 1 kN and 5 kN, making this application perfect for a single column test frame such as Instron's 34SC or 68SC. If the adhesive requires a higher capacity system, Instron’s dual column table model frames are available up to 50 kN.

EN 1465 Test Setup
1. Instron 34SC-05
2. Bluehill Universal Dashboard (2490-696)
3. 2530 Series Load Cell (2530-100N)
4. 500 N Screw Side-Action Grips (2710-112)
Both pneumatic side-action grips and advanced screw side-action grips are excellent gripping choices for this standard. Both types of grips are adjustable in order to offset the jaw faces and ensure that the lap joint remains centered, and both feature quick-change jaw faces that can be easily changed to accommodate different materials.
- When testing lap shear specimens, the lap joint causes the two ends of the specimen to be offset from the vertical load line of the test. In order to ensure that the specimen remains centered in the load string and yields a true shear force calculation, the grips must have offset jaw faces to ensure they are directly aligned with the plane of the adhesive bond.
- EN 1465 requires reporting the breaking force or strength, however, it is important to remember that shear strength is calculated by dividing the breaking force by the adhesive bond area.
- Users who purchase Instron's Bluehill Universal software are provided with one free application module upon purchase. Each module contains pre-configured test methods and supporting documentation to assist with testing to various standards, including EN 1465 which is part of the Adhesives module.
6800 Catálogo de sistemas de ensayo Serie Premier
Los sistemas de ensayo universales Serie 6800 de Instron proporcionan una precisión y fiabilidad sin igual. Construida sobre una arquitectura de sistema Operator Protect pendiente de patente, con un kit Smart-Close totalmente nuevo y funciones de mitigación de colisiones, la Serie 6800 hace que los ensayos de materiales sean más sencillos, limpios y seguros que nunca.
Serie 3400: soluciones de ensayo asequibles
Sistemas de ensayo universales Serie 3400 de Instron para ensayos de tracción, compresión, doblado y otros materiales.
Catálogo de Bluehill Universal
El software Bluehill Universal está diseñado desde el principio para una interacción táctil y una experiencia de usuario intuitiva. Descubre ensayos más sencillos y limpios con funciones como métodos de ensayo precargados, QuickTest en segundos, exportación de datos mejorada e Instron Connect, una nueva función que proporciona un enlace de comunicación directa con el servicio. Los usuarios de versiones anteriores del software, como Bluehill 2 y Bluehill 3, pueden actualizarse fácilmente a la última versión de Bluehill.
Mordazas neumáticas de acción lateral Serie 2712-04X
Las mordazas neumáticas de acción lateral ofrecen una solución de agarre versátil para una amplia gama de materiales. Capacidades nominales entre 1 y 10 kN.
Serie 2710 Mordazas de acción de tornillo
Las Mordazas de acción de tornillo proporcionan un método sencillo y eficaz para sujetar muestras de ensayo en una amplia gama de aplicaciones.