O Ring Spindles
Different O-Ring diameters and thicknesses require different spindles in order to provide more accurate tests. The spindle is the component which hooks inside the O-Ring and pulls on it during test.
The spindles must be used in conjunction with a suitable O-ring test fixture.The spindles come in different sizes specified by testing standards or by a specific need.
The main fixture remains on the system and the spindles can be easily interchanged to accommodate the specimen.Tensile testing of elastomeric rings to a variety of International Standards
Principe de fonctionnement
The spindles come in different sizes specified by testing standards or by a specific need. The main fixture remains on the system and the spindles can be easily interchanged to accommodate the specimen.Applications
Different O-Ring diameters and thicknesses require different spindles in order to provide more accurate tests. The spindle is the component which hooks inside the O-Ring and pulls on it during test. The spindles must be used in conjunction with a suitable O-ring test fixture.Accessories
Article | Roller Diameter | Roller Width | Cat # |
---|---|---|---|
Spindle Set - 1/8 in | 3.175 mm 0.125 in | 7 mm 0.28 in | 2717-074 |
Spindle Set - 1/4 in | 6.35 mm 0.25 in | 7 mm 0.28 in | 2717-075 |
Spindle Set per ASTM D1414 | 12.7 mm 0.5 in | 7 mm 0.28 in | 2717-076 |
Spindle Set per ASTM D412 | 4.75 mm 0.19 in | 7 mm 0.28 in | 2717-070 |
Spindle Set per BS 3704 | 15 mm 0.59 in | 25 mm 0.98 in | 2717-071 |
Spindle Set per DIN 53504 R1 | 22.3 mm 0.88 in | 7 mm 0.28 in | 2717-072 |
Spindle Set per DIN 53504 R2 | 18.3 mm 0.72 in | 7 mm 0.28 in | 2717-073 |