50kN Wood Bend Fixture Base Beam (800mm max.span)
2820-041 | Bend Fixture Lower Beam for Wood and Fiberboard
Capacity: 50 kN (5,000 Kgf, 11,250 lbf).
Maximum Span: 800 mm (31.5 in)
Temperature Range: Ambient only
Lower fitting: 4 x M10 ( on 90 mm x 280 mm spacing)
Features:
- Graduated scale for ease of anvil span setting
- High strength steel construction
- Compatible with full range of optional anvils, four point upper beams and deflectometer
Requires optional anvil set(s)
Meets:
JIS A5905, JIS A5906, JIS A5908, JAS 112, JAS 601,BS 373, BS 5669, EN 310, EN 789, ISO 3133,ASTM D 1037 and ASTM D 143 testing standards with suitable optional anvil sets/four-point upper beams/deflectometer
Masse | 36.6 kg (80.1 lb) |
---|---|
Capacité | 50 kN (11,250 lbf) |
Fixation inférieure | 4 x M10 Bolts (90 x 280 mm) |
Support Span | 800 Max. mm (31.5 Max. in) |
Normes d'essais | See Anvils for compliance with standards |
- 50kN Four-Point Upper Beam for use with Bend Fixture Lower Base Beam
- 3 point Rigid Anvil set. 20mm dia. upper, 20mm dia. Lower
- 3 point Rigid Anvil Set
- 3 point Rigid Anvil Set. 76mm dia. Upper, 76mm dia. Lower
- 3 point Rigid Anvil set. 60mm dia. upper, 60mm dia. lower.
- 4 Point Rigid Anvil Set
- 3 Point Articulating and Rolling Anvil Set
- 3 point Anvil Set
- 3 Point Anvil Set
- 4 Point Upper Anvil Set
- 3 Point Anvil Set
- 4 Point Upper Anvil Set
- 3 Point Articulating and Rolling Anvil Set
- Yoke Deflectometer for use with 2820-040, -041 and -042 Bend Fixtures
Bend Test Fixtures For Wood | 2820-04x
Bend tests provide a quick and simple way to determine the strength and deformation properties of wood and timber products. The test is also particularly relevent in this application because wood is frequently used in the form of beams where resistance to bending is an important parameter. A range of fixtures is available to cater for various specimen sizes and strengths. All fixtures can be equipped with a range of optional support rollers some of which feature articulation to cater for warped specimens.The range of fixtures is ideal for tests on MDF and fiberboard as well as natural timber.
- Produits
- 11/19/2008
- 0.6 MB