2820-056 | 3 point Articulating and Rolling Anvil Set
Upper anvil; Rigid wood block, 76 mm rad., 70 mm wide
Lower; Bearing plate, 90 x 90 mm
Meets: ASTM D 3043, ASTM D 143.
Upper fitting: 6 mm clevis (Type Om) and 0.5 in clevis (Type Dm)