Internal Bond Test Fixture for Chipboard and Fiberboard
2820-061 | Internal Bond Grips for Chipboard and Fiberboard
Capacity: 10 kN (1,000 Kgf, 2,250 lbf).
Temperature Range: Ambient only
Upper fitting: 6mm clevis (Type Om) swivel
Lower fitting: 0.5in clevis (Type Dm)
Features:
- Integral swivel upper connection
- Rotatable lower grip for ease of specimen insertion
Requires: 2820-062 specimen blocks.
Meets:
ASTM D 1037-99, BS 5669-1979, JIS A5905-1994, JIS A5906-1983, JIS A5908-1994
Masse | 0.65 (upper without specimen block) kg (1.4 (upper without specimen block) lb) |
---|---|
Largeur | 66 mm (2.6 in) |
Capacité | 10 kN (2250 lbf) |
Fixation inférieure | 0.5 in clevis (Type Dm) |
Longueur de l'éprouvette | 50 mm (2 in) |
Epaisseur de l'éprouvette | As required mm (As required in) |
Largeur de l'éprouvette | 50 mm (2 in) |
Normes d'essais | ASTM D1037-99, BS 5669-1979, JIS A5905-1994, JIS A5906-1983, JIS A5908-1994 |
Upper Effective Length | 57 mm (2.2 in) |
Upper Fitting | 6mm clevis (Type Om) swivel |
Internal Bond Fixture For Wood | 2820-061
The 2820-061 internal bond fixture is designed for testing the strength properties of wood or adhesive bonds in wood by tensile loading. The fixture consists of a self-aligning upper grip and a rotatable lower grip. Tensile loading is applied to the specimen via blocks bonded to the specimen itself. Simple clevis pin interfaces are used which allow quick and easy fitting and removal of the grips.