Compression Platen - Spherically Seated-Diameter 165 mm (6.5 in)
W-2005-C | Compression Platen - Spherically Seated
- Diameter: 165 mm (6.5 in)
- Capacity (Load): 4500 kN (1,000,000 lbf)
- Effective Height: 101.6 mm (4 in)
- Approximate Weight: 17 kgs (37.4 lbs)
- Attachment: Type R1m (1.0 in) holding button
Diamètre | 165 mm (6.5 in) |
---|---|
Hauteur | 101.6 mm (4.0 in) |
Masse | 17 kg (37.4 lb) |
Capacité | 4500 kN (1,000,000 lbf) |
Pressure Rating | 690 MPa (100,000 psi) |
Upper Fitting | R1M |
Compression Platens W-2004 and W-2005 Series
Instron® Industrial Series Compression Platens are designed to maximize compression testing performance. These high-strength, versatile platens are available in both plane and self-aligning models, and can be easily configured with Instron and other static universal testing machines.