Pin and Clevis Holders 4 mm slot 4 mm pin
Pin and Clevis Specimen Holders
Size: 4 mm slot, 4 mm pin
Temperature: 1100 Degrees C (2000 Degrees F)
Upper and Lower Fittings: US Customary 3/4 in-10 (Type R3f)
Material: Iconel 713-C
Coupling Length: 69.9 mm (2.75 in)
Coupling Diameter: 28.6 mm (1.125 in)
Note: Using a specimen that is smaller (thinner) than the slot width specified for a given set of holders can result in misalignment of the specimen.
Gamme de températures | 1100°C (2000°F) |
---|