0.50 Inch Shoulder-End Specimen Inserts, 400 kN
W-5159-A1 | 0.50 Inch Shoulder-End Specimen Inserts, 400 kN
0.50 inch shoulder-end specimen inserts, One set, ASTM A48
Static Tensile Capacity: 400kN
Instron standard specimen drawing 232572-2
Reference ASTM A48, Figure 1, Specimen A
Requirement: W-5159 600kN Insert Holder
Capacité | 400 kN (89,900 lbf) |
---|---|
Static or Fatigue Rated | Static |
Gamme de températures | 0-38°C (32-100°F) |
Split Insert Tensile Grips W-5158 and W-5159
Instron® Split Insert Tensile Grips are designed for safe, high-volume production testing of shoulder-end or button-head machined specimens. Engineered with an operator focus, the split insert style tensile grips are easy to install, offer quick change inserts for standard specimen sizes, and promote efficient testing of a wide range of metals and alloys.
- Produits