ASTM F2516 Tensile Testing of Nitinol Wire
ASTM F2516 measures the tensile properties of superelastic nickel-titanium or Nitinol. The material properties of nitinol are different from those of most other materials – nitinol will change its structure depending on its temperature or the amount of stress applied to it. This means that it will exhibit very different stress strain profiles during loading and unloading, which is why this standard captures both an upper and lower plateau strength, rather than a singular yield strength. The ASTM F2516 test method is designed to pull the material in tension to 6% strain, then unload the material to a value of less than 7MPa before being pulling it to failure.
- Metals
- Biomedical
- Tension
- Compression
- ASTM F2516
Nitinol's unique properties mean that it is used extensively in the biomedical industry to create stents, dental wires, catheter guidewires, internal fracture fixation devices, and biopsy forceps. One of its properties - shape memory - enables it to "remember" its shape when formed at a certain temperature. When the temperature is lowered beyond this point Nitinol can be molded to any other shape, but will automatically revert to its original shape once it reaches the temperature at which it was initially formed. This property makes it extremely useful for the creation of stents, which are used to hold open blood vessels and prevent severe clots. The stent can be transported through the body to the target location in a compacted form, reforming to its original cylindrical form once it warms up to body temperature at the target location. Nitinol is also commonly used for braces – the Nitinol is molded into the desired final shape, and the temperature within the mouth stresses the material to reform, slowly adjusting the teeth into their ideal positions. Unlike more traditional braces, nitinol braces wire is especially beneficial because it does not require frequent retightening.
Test SetupASTM F2516 is typically performed on a dual column materials testing system such as Instron's 6800 Series. A 5 kN load cell is most likely appropriate for most materials. Bluehill Universal software with TestProfiler is also required, and the test method for ASTM F2516 comes pre-loaded in Bluehill Universal's Biomedical Applications Module.
ASTM F2516 Test Setup | |
---|---|
1) | 6800 Series Universal Testing System |
2) | Bluehill Universal Software |
3) | 2580 Series Load Cell |
4) | 2714-005 Pneumatic Cord and Yarn Grips |

The gripping solution is dictated by specimen diameter, with most small diameters being tested with pneumatic cord and yarn grips and larger diameters utilizing pneumatic side action grips with serrated faces.
The diameter of the wire being tested determines the extensometry class required. For any wire 0.2 mm or smaller in diameter, crosshead movement can be used for strain measurement. Diameters greater than 0.2mm require a class C extensometer, with Instron's AUTOX automatic contacting extensometer, and AVE2 non-contacting extensometers being popular choices, as the weight of clip-on devices can affect results when testing such small specimens.
Specimen diameter and gauge length also determine test speed, so utilizing expression builder in Bluehill Universal can provide an easy way to update the test speed automatically. The lab temperature for this test is also very important - the material needs to be tested at a temperature at least 5 degrees higher than its austenitic finish transformation temperature. If not, the material will be partially transformed to a different material state, affecting the results.
Related ContentSérie 6800 Brochure sur les systèmes d’essai de première qualité
Les systèmes d'essai universels Instron série 6800 offrent une précision et une fiabilité inégalées. Construit sur une architecture système Operator Protect en instance de brevet avec un tout nouveau kit de régulation d’air Smart-Close et des fonctions d’atténuation des collisions, la série 6800 rend les essais de matériaux plus simples, plus intelligents et plus sûrs que jamais.
Solutions d'essai abordables - Série 3400
Systèmes d'essai universels Instron série 3400 pour les essais de traction, de compression, de flexion et autres essais de propriété des matériaux.
Brochure de Bluehill Universal
Le logiciel Bluehill Universal est conçu dès le départ pour une interaction tactile et une expérience utilisateur intuitive. Vous découvrirez que les essais deviennent plus simples et plus intelligents grâce à des fonctionnalités, telles que les méthodes d’essais préconfigurées, le QuickTest fait en quelques secondes, l’exportation de données optimisée et Instron Connect - une nouvelle fonctionnalité qui fournit un lien de communication direct avec le service technique. Les utilisateurs des versions précédentes du logiciel, telles que Bluehill 2 et Bluehill 3, peuvent facilement faire la mise à jour à la toute dernière version de Bluehill.
TestProfiler pour Bluehill Universal
Amarrages pneumatiques à action latérale - Série et modèles 2712-04X
Les amarrages pneumatiques à action latérale constituent une solution polyvalente pour un large éventail de matériaux. Capacités nominales comprises entre 1 et 10 kN.
Amarrages pneumatiques pour cordes et fil textile - Modèle 2714-005
Les amarrages pneumatiques pour cordons et fils constituent une méthode pratique pour serrer les fibres, les cordons, les fils et les fils fins pour réduire les problèmes associés aux essais de ces types de matériaux. Capacité nominale 1 kN.
Extensiomètre vidéo sans contact AVE 2
La deuxième génération d’extensomètre vidéo avancé (AVE 2) utilise une nouvelle technologie brevetée pour la mesure de la déformation sans contact, ce qui en fait le plus rapide et le plus précis disponible dans le commerce.
Extensiomètre automatique avec contact - Modèle AutoX 750
L’AutoX 750 est un extensomètre automatique avec contact à haute résolution et à grande portée. Il peut être monté sur tous les systèmes électromécaniques 3300, 3400, 5500, 5900, ou 6800 de table et de sol, ainsi que sur les systèmes d’essais hydrauliques statiques LX, DX, HDX et KPX. Il est bien adapté aux applications impliquant les plastiques, les métaux, le biomédical, les composites, les élastomères, et plus encore. L’AutoX a une course maximale de 750 mm et une précision de ± 1 µm.