ASTM D1894-14 Coefficient of Friction of Plastic Film

ASTM D1894

ASTM D1894 is a standardized test method used for determining static (μ_s ) and kinetic (μ_k ) coefficients of friction of plastic film and sheeting. Plastic film is a widely used material in the packaging industry and includes many types of food packaging (produce bags, carton liners, meat seal wrap) and non-food packaging (envelope liners, potting soil sacks). Plastic films are also key components of more complex products, such as electric vehicle batteries. In order to ensure that they perform as expected for the end user, the frictional properties of these films must be characterized and controlled. 

Separator Film Testing for Electric Vehicle Batteries

ev battery icon  

Separator films are used in EV battery production to separate the anode and cathode in lithium-ion and other liquid electrolyte batteries. These films are required in high volumes and are extremely critical to product safety. Because testing standards specific to EV batteries have not yet been established, ASTM D1894 is commonly used as a proxy standard to characterize their frictional properties. The most common material used for separator film is polyolefin, a polymer film that is strong enough to withstand the winding operation during assembly as well as uneven plating of lithium on the anode due to extensive use. Safer and stronger separator material more effectively prevents contact between the anode and cathode, while thinner material helps reduce the weight of each battery and improve energy density. Understanding the frictional properties of this polymer film can help ensure the material is being wound properly during assembly and will behave as expected under extensive use.

Materials Testing System 

When testing thin films to ASTM D1894 it is important to use a test machine with a high data capture rate. Because test events can happen quickly, a machine with a low data capture rate may miss key peaks and troughs in the data, leading to an inaccurate average strength value. Instron’s 6800 series test frames are capable of data capture up to 5 kHz to ensure that all test events are captured. For ASTM D1894 testing we recommend a 6800 series single column frame equipped with a low force (5 – 100 N) 2530 series load cell (depending on the expected frictional forces).




ASTM D1894 Test Setup
6800 Series Universal Testing System
 Bluehill Universal Software
 2530 Series Load Cell
2810-005 Coefficient of Friction Fixture

 

ASTM D1894 coefficient of friction films

HOW TO PERFORM A TEST TO ASTM D1894


This test requires the use of Instron's 2810-005 Coefficient of Friction fixture, which is specifically designed to meet the requirements of ASTM D1894 and ISO 8295. The film under test is secured on a flat surface and a sled of known weight is wrapped in the same material. The motion of the crosshead drags the sled along the film being tested and the force measured is used to determine both the static and kinetic coefficients of friction. Complete details on how to perform this test can be found by reading the full  ASTM D1894 standard.

Tips and Tricks
  • Instron’s 2530 series load cells can maintain accuracy down to 1/500th of the cell’s capacity when used on a 6800 Series universal testing system. The lowest capacity 2530 series load cell is 5 N, meaning it can maintain 1% accuracy from 0.02 N to 5 N. Forces beneath the lower limits can be measured, but Instron cannot guarantee stated accuracy.
  • Instron's Bluehill Universal testing software has advance pre-built methods available for ASTM D1894 to ensure that your test speeds and calculations are compliant.
Related Content

Série 6800 Systèmes d'essai universels

Les systèmes d'essais universels Instron série 6800 offrent une précision et une fiabilité inégalées. Construit sur une architecture système Operator Protect en instance de brevet avec un tout nouveau kit de régulation d’air Smart-Close et des fonctions d’atténuation des collisions, la série 6800 rend les essais de matériaux plus simples, plus intelligents et plus sûrs que jamais.

Brochure Bluehill Universal

Le logiciel Bluehill Universal est intégralement conçu pour une interaction tactile et une expérience utilisateur intuitive. Vous découvrirez que les essais deviennent plus simples et plus intelligents grâce à des fonctionnalités, telles que les méthodes d’essais préconfigurées, le QuickTest fait en quelques secondes, l’exportation de données optimisée et Instron Connect - une nouvelle fonctionnalité qui fournit un lien de communication direct avec le service technique. Les utilisateurs des versions précédentes du logiciel, telles que Bluehill 2 et Bluehill 3, peuvent facilement faire la mise à jour à la toute dernière version de Bluehill.

Dispositif d’essai pour coefficient de friction - Série 2810-005

Le dispositif de mesure du coefficient de friction Instron 2810-005 est un dispositif d’essai permettant de mesurer le coefficient de friction statique et cinétique des films et feuilles en plastique selon la norme ASTM D 1894 ou la norme ISO 8295.

Cellules de charge - Série 2580

Les cellules de charge de la série 2580 sont spécifiquement conçues pour être utilisées avec les systèmes d’essais des séries 5900 et 6800. Elles offrent des performances exceptionnelles avec la possibilité de mesurer des forces aussi faibles que 1/1000e de la capacité de force avec une précision de lecture de 0,5 %.

Cellules de faible charge - Série 2530

Les cellules de charge de la série Instron 2530 sont spécialement conçues pour être utilisées avec tous les systèmes d’analyse de faible charge d’Instron. Les capacités de force vont de ±5 à ±100 N (0,5 à 10 kgf, 1,12 à 22,5 lbf) avec une large plage de mesure permettant de mesurer la force jusqu’à 1/500e de la capacité de la cellule de charge.