ASTM D2256 - Standard Test Method for Tensile Properties of Yarns by the Single-Strand Method

ASTM D2256 tensile testing of yarn

ASTM D2256 is a testing standard that specifies the method for determining the tensile properties of monofilament, multifilament, and spun yarns. It provides a testing procedure for determining maximum force and elongation and provides directions for calculating other properties such as breaking tenacity and modulus. ASTM D2256 is intended to determine the quality of the raw material while aiding in quality control of the finished product.

Materials Testing System

Due to its high data capture rate, we recommend our high tier 6800 Series test frame as the optimal solution for ASTM D2256 testing, although our more affordable 3400 Series is also appropriate. A single column frame is adequate for most single-strand yarn specimens as the loads rarely exceed 5 kN. In cases where yarn specimens require greater force, a dual column system may be needed.




ASTM D2256 Test Setup
1) 6800 Series Universal Testing System
2) Bluehill Universal Software
3) 2580 Series Load Cell
4) 2714-005 Pneumatic Cord and Yarn Grips

 

ASTM D2256 system setup
Grips

The most common gripping solution for ASTM D2256 are pneumatic cord and yarn grips with smooth clamping blocks, which are well suited for testing nearly all types of yarn specimens while maintaining high throughput. A specially designed horn with a smooth finish and a contoured surface with a graduated cam allows for easy loading and a stress reduced clamping area on the specimen. By incorporating a design that evenly distributes gripping force over the surface of a curved half capstan, the chances of specimen failures are reduced. 

Instron’s 2 kN capacity cord and yarn grips can also be paired with jaw faces with several other finishes to provide adequate clamping and avoid damage to the specimens during testing. The pneumatic grips allow users to fine-tune the gripping pressure in order to avoid jaw breaks or slippage. In some cases with strong or slippery yarn specimens, use of extra padding material within the clamping blocks, such as paper or emery cloth, can also be helpful.

2714-005
1 kN Model | 2714-005

TIPS AND TRICKS


  • ASTM D2256 is available as a pre-built test method within Bluehill Universal software. This method includes pre-configured calculations to help expedite test setup and simplify the testing process.

  • This standard recommends a Constant Rate of Extension (CRE) test frame for operating at a 20 second time-to-break, paired with grips that provide adequate clamping throughout testing. If the frame cannot provide a 20 second time-to-break or the grips allow for slippage while testing, the standard allows for alternative testing methods. These alternatives will likely be dependent on each yarn’s material properties.
Related Content

Série 6800 Systèmes d'essai universels

Les systèmes d'essais universels Instron série 6800 offrent une précision et une fiabilité inégalées. Construit sur une architecture système Operator Protect en instance de brevet avec un tout nouveau kit de régulation d’air Smart-Close et des fonctions d’atténuation des collisions, la série 6800 rend les essais de matériaux plus simples, plus intelligents et plus sûrs que jamais.

Amarrages pneumatiques pour cordes et fil textile - Modèle 2714-005

Les amarrages pneumatiques pour cordons et fils constituent une méthode pratique pour serrer les fibres, les cordons, les fils et les fils fins pour réduire les problèmes associés aux essais de ces types de matériaux. Capacité nominale 1 kN.

Amarrages pneumatiques pour cordes et fil textile - Modèle 2714-040

Les amarrages pneumatiques pour cordons et fils constituent une méthode pratique pour serrer les fibres, les cordons, les fils et les fils fins pour réduire les problèmes associés aux essais de ces types de matériaux. Capacité nominale 2 kN.

Brochure Bluehill Universal

Le logiciel Bluehill Universal est intégralement conçu pour une interaction tactile et une expérience utilisateur intuitive. Vous découvrirez que les essais deviennent plus simples et plus intelligents grâce à des fonctionnalités, telles que les méthodes d’essais préconfigurées, le QuickTest fait en quelques secondes, l’exportation de données optimisée et Instron Connect - une nouvelle fonctionnalité qui fournit un lien de communication direct avec le service technique. Les utilisateurs des versions précédentes du logiciel, telles que Bluehill 2 et Bluehill 3, peuvent facilement faire la mise à jour à la toute dernière version de Bluehill.