ASTM D575-91: Standard Test Methods for Rubber Properties in Compression
- Elastomers
- Compression
- ASTM D575
ASTM D575 is a testing standard used to determine the stiffness of rubber materials in compression. ASTM D575 allows rubber suppliers to characterize the stiffness of the material they produce to help downstream manufacturers source the correct material for their components. Data collected from ASTM D575 testing is important for applications that require elastomeric materials subjected to compressive stresses. One wide-ranging application is the sealant industry, as due to its ease of extrusion and flexible nature, rubber is commonly used material for sealants.
Method A applies a predetermined deflection to the cylindrical specimen at which the force is recorded. Alternatively, Method B applies predetermined minor and major forces to the specimen and deflection is measured.
Materials Testing SystemDepending on maximum expected forces, ASTM D575 is performed on a single column or dual column universal testing system such as Instron's 3400 and 6800 Series systems. This system setup requires a matching load cell and upper and lower platens with diameters larger than the diameter of the specimen. Platens should have rigid connections to the frame and load cell, and must be rated to a load capacity which exceeds forces generated during the test.ASTM D575 Test Setup | |
---|---|
1) | 3400 Series Universal Testing System |
2) | Bluehill Universal Software |
3) | 2530 Series Load Cell |
4) | 2501 Series Compression Platens |

Though not required by the standard, parallelism can be ensured by including an integral spherical seat on the upper platen. Though crosshead displacement measurements are adequate for ASTM D575, those interested in the most accurate deflection measurement should consider using a 2601-04x Series linear variable displacement transducer.
ASTM D575 Accessories | |
---|---|
1) | Self-Aligning Spherical Seat |
2) | 2601-04x Series LVDT |

- For the most accurate deflection measurements, we recommend a 2601 series LVDT attached to the platen itself over the use of crosshead displacement measurement. If crosshead position is used, it is important to use Corrected Displacement in Bluehill Universal to prevent error from machine compliance.
- Is parallelism of platens important to your lab? If so, compression platens with integral spherical seats are ideal for ensuring platen to platen parallelism.
- If performing ASTM D575 Method B with an Instron machine, be aware that a force hold is a requirement of the test. Similar to longer creep or stress-relaxation tests, holding force requires the load cell’s transducer settings to be tuned to the effective stiffness of test setup, which includes the specimen itself and any fixturing.
Série 6800 Brochure sur les systèmes d’essai de première qualité
Les systèmes d'essai universels Instron série 6800 offrent une précision et une fiabilité inégalées. Construit sur une architecture système Operator Protect en instance de brevet avec un tout nouveau kit de régulation d’air Smart-Close et des fonctions d’atténuation des collisions, la série 6800 rend les essais de matériaux plus simples, plus intelligents et plus sûrs que jamais.
Solutions d'essai abordables - Série 3400
Systèmes d'essai universels Instron série 3400 pour les essais de traction, de compression, de flexion et autres essais de propriété des matériaux.
Brochure de Bluehill Universal
Le logiciel Bluehill Universal est conçu dès le départ pour une interaction tactile et une expérience utilisateur intuitive. Vous découvrirez que les essais deviennent plus simples et plus intelligents grâce à des fonctionnalités, telles que les méthodes d’essais préconfigurées, le QuickTest fait en quelques secondes, l’exportation de données optimisée et Instron Connect - une nouvelle fonctionnalité qui fournit un lien de communication direct avec le service technique. Les utilisateurs des versions précédentes du logiciel, telles que Bluehill 2 et Bluehill 3, peuvent facilement faire la mise à jour à la toute dernière version de Bluehill.
Plateaux de compression - Série 2501
Ces plateaux de compression faciles à installer sont des dispositifs usinés avec précision, conçus pour une distribution uniforme des charges de compression pendant un essai.
Capteurs de déflexion LVDT - Série 2601
Les transducteurs différentiels variables linéaires (LVDT) ou transformateurs linéaires différentiels variables de la série 2601 sont des dispositifs de mesure qui mesurent le déplacement des bâtis de charges.