ASTM D5766 Open-Hole Tensile Strength of Polymer Matrix Composite Laminates
- Composites
- Tension
- ASTM D5766
ASTM D5766 determines the open-hole tensile strength of multidirectional composite coupons. The composite coupon geometry has to be in accordance with test method ASTM D3039. ASTM D5766 is designed to produce tensile results on multidirectional polymer matrix composite laminates mainly used in the aerospace industry for material specifications, research and development, quality assurance, and structural design and analysis.
Materials Testing System
Because the forces required for ASTM D5766 testing are relatively high, a floor model universal testing system such as Instron's 5980 Series is recommended. The properties of composite materials are highly directional, making it especially necessary to test with a system that is well-aligned and repeatable. An AlignPRO fixture and precision manual or hydraulic wedge grips are necessary in order to test specimens within alignment requirements and without slippage.
ASTM D5766 Test Setup | |
---|---|
1) | 5980 Series Universal Testing System |
2) | Bluehill Universal Software |
3) | AlignPRO Fixture |
4) | 2580 Series Load Cell |
4) | 2716-030 Precision Manual Wedge Grips |

- This testing is performed in accordance with ASTM D3039, but instead of a uniform coupon, the specimen is modified with a centrally-located hole. When calculating the ultimate tensile strength based on the cross sectional area, the hole's presence is disregarded.
- ASTM D5766 requires that the specimen coupon have multidirectional fiber orientations in a minimum of two directions. Typical test results include the ultimate tensile strength, the width of specimen-to-hole diameter ratio, hole-diameter-to-coupon-thickness ratio, and, if desired, the edgewise percent bending in accordance with ASTM D3039.
- The only valid failure mode in determining the ultimate tensile strength is one that passes through the prefabricated hole in the test coupon. A break outside of this location does not deliver valid test results.
Brochure sur les essais de composites
Brochure sur les machines d'essai universelles à force élevée
Les systèmes à force élevée d’Instron comprennent des systèmes d’essais électromécaniques et hydrauliques à haute capacité. pour les applications de traction et de compression. Les capacités de force vont de 100 kN à 2000 kN.
Système d’alignement AlignPRO
Modèle au sol à doubles colonnes - Série 5980
Les modèles de sol de série 5980 sont couramment utilisés pour les essais les métaux et alliages à haute résistance, les composites avancés, les structures aérospatiales et automobiles, les boulons, les fixations et les aciers en plaques.
2743-401 hydraulique à étau Amarrages
Les amarrages hydrauliques à étau 100 kN d’Instron fournissent une solution innovante pour les essais haute capacité et offrent des performances de préhension, une facilité d’utilisation et une sécurité de l’opérateur améliorées.
Amarrages manuels de précision à étau - Série 2716
Disponibles en capacités de 100 kN et 250 kN, les amarrages manuels de précision à étau 2716-028/30 d’Instron offrent un serrage fiable pour une large gamme de matériaux ainsi qu’un alignement reproductible qui répond aux exigences de Nadcap.