ASTM D6641 - Compressive Properties of Polymer Matrix Composite Materials Using a Combined Loading Compression (CLC) Test Fixture

ASTM D6641

ASTM D6641 is a testing standard that determines the compressive strength and stiffness properties of polymer matrix composite materials using a combined loading compression (CLC) test fixture. This test method is designed to produce compressive property data on polymer matrix - mainly used in the Aerospace industry - for the purposes  of research and development, quality assurance, and structural design and analysis. ASTM D6641 can be used to test unidirectional (0° ply orientation) composites as well as multi-directional composite laminates, fabric composites, chopped fiber composites, and similar materials.

Test Fixture 

A CLC test fixture such as Instron's CP104483 is necessary for performing ASTM D6641 testing. The fixture is placed between two compression platens which initiate the compressive force onto the fixture, which in turn subjects the specimen to a combination of Shear- and End-Loading.

 

ASTM D6641 test fixture

 

Materials Testing System

ASTM D6641 is best performed on a high force universal testing system such as Instron's 6800 Series electromechanical systems with Bluehill Universal software. Though most composites can be tested with a 250kN capacity system, labs testing a wider range of materials may benefit from a higher capacity system. An AlignPRO fixture should be used to ensure accurate results. 




ASTM D6641 Test Setup
 6800 Series Universal Testing System
Bluehill Universal Software
2580 Series Load Cell
CP104483 Custom Test Fixture
AlignPro

 

ASTM D6641 test setup 
Tips and Tricks
  • The specimen may be untabbed (Procedure A) or tabbed (Procedure B), as required. One requirement for a successful test is that the specimen ends do not crush during the test. Untabbed specimens are usually suitable for use with materials of low orthotropy: for example, fabrics, chopped fiber composites, and laminates with a maximum of 50% 0° plies, or equivalent. Materials of higher orthotropy, including unidirectional composites, typically require tabs.
  • The most important results are the compressive strength, the compressive strain and the compressive Poisson’s ratio determined by Chord method. In addition to these calculations, the failure mode of each specimen is documented with the appropriate failure code as described within the standard.
  • For more information, purchase ASTM D6641.
Related Content

Brochure sur les systèmes d’essais de première qualité de la série 6800

Les systèmes d'essais universels Instron série 6800 offrent une précision et une fiabilité inégalées. Construit sur une architecture système Operator Protect en instance de brevet avec un tout nouveau kit de régulation d’air Smart-Close et des fonctions d’atténuation des collisions, la série 6800 rend les essais de matériaux plus simples, plus intelligents et plus sûrs que jamais.

Dispositifs d’essai des composites - compression

Instron propose plusieurs dispositifs pour les essais de compression des composites sans plaques de guidage anti-flambage. C’est souvent le moyen privilégié pour les essais sur composites, car la longueur libre non supportée est plus représentative du véritable comportement en compression.

Brochure de Bluehill Universal

Le logiciel Bluehill Universal est conçu dès le départ pour une interaction tactile et une expérience utilisateur intuitive. Vous découvrirez que les essais deviennent plus simples et plus intelligents grâce à des fonctionnalités, telles que les méthodes d’essais préconfigurées, le QuickTest fait en quelques secondes, l’exportation de données optimisée et Instron Connect - une nouvelle fonctionnalité qui fournit un lien de communication direct avec le service technique. Les utilisateurs des versions précédentes du logiciel, telles que Bluehill 2 et Bluehill 3, peuvent facilement faire la mise à jour à la toute dernière version de Bluehill.

Système d’alignement AlignPRO

Le système AlignPROTM d’Instron est conçu pour aider les opérateurs de la machine à mesurer et ajuster l’alignement des chaînes de charge.