ISO 11339 T-Peel Test Flexible to Flexible Bonded Assemblies

ISO 11339 peel test

ISO 11339 measures the comparative peel properties of adhesive bonds between flexible adherends by using a T-peel test. The test is referred to as a “T-peel” due to the shape the two flexible adherends form as they are pulled apart. Average peel strength for each specimen type and average, minimum, and maximum peeling loads for each individual specimen are the primary results of interest. Manufacturers use this standard for quality control in a wide range of industries as it is primarily intended for determining relative peel resistance between individual specimens or different types of adhesives. Direct comparison of different adhesives can only be made when specimen construction and test conditions are identical.

ISO 11339 Test Setup 

For peel tests, it is critical to use a high data acquisition rate to capture all peaks and troughs in order to ensure all test events are represented in the results. Too low of a bandwidth may “dull” the results and lead to artificially low peel strength values. For this reason, we recommend an Instron 6800 series test frame, which enables a data capture rate of up to 5 kHz. System capacity will depend on the strength of the adhesive; however, many tests to this standard will fall below 5 kN capacity, making a single column frame (68SC) ideal. If the adhesive requires a higher capacity system, Instron’s dual column table model frames are available up to 50 kN.




ISO 11339 Test Setup
1) 6800 Series Universal Testing System
2) Bluehill Universal Software
3) 2580 Series Load Cell
4) 2712-041 (1 kN) Pneumatic Side-Action Grips

 

ISO 11339 peel test of adhesive bonds
Grips 

Pneumatic side action grips prevent specimen slippage by maintaining a constant clamping pressure throughout testing. They are available in capacities from 50N to 10kN, appropriate for the full range of adhesive strengths. Both advanced side action grips and pneumatic grips feature quick-change jaw faces that can be easily changed to accommodate different materials.

250 N Model | 2712-052
2710-112
500 N Model | 2710-112
Tips and Tricks
  • When performing an ISO 11339 test, the two adherends do not need to be the same material or thickness. However, if one adherend is more flexible than the other, attach the less flexible one to the moveable (top) grip.
  • Bluehill Universal software comes with with one free application module upon purchase. Each module contains pre-configured test methods and supporting documentation to assist with testing to various standards. ISO 11339 is included as part of the Adhesives module.
Related Content

Série 6800 Brochure sur les systèmes d’essai de première qualité

Les systèmes d'essai universels Instron série 6800 offrent une précision et une fiabilité inégalées. Construit sur une architecture système Operator Protect en instance de brevet avec un tout nouveau kit de régulation d’air Smart-Close et des fonctions d’atténuation des collisions, la série 6800 rend les essais de matériaux plus simples, plus intelligents et plus sûrs que jamais.

Solutions d'essai abordables - Série 3400

Systèmes d'essai universels Instron série 3400 pour les essais de traction, de compression, de flexion et autres essais de propriété des matériaux.

Brochure de Bluehill Universal

Le logiciel Bluehill Universal est conçu dès le départ pour une interaction tactile et une expérience utilisateur intuitive. Vous découvrirez que les essais deviennent plus simples et plus intelligents grâce à des fonctionnalités, telles que les méthodes d’essais préconfigurées, le QuickTest fait en quelques secondes, l’exportation de données optimisée et Instron Connect - une nouvelle fonctionnalité qui fournit un lien de communication direct avec le service technique. Les utilisateurs des versions précédentes du logiciel, telles que Bluehill 2 et Bluehill 3, peuvent facilement faire la mise à jour à la toute dernière version de Bluehill.

Amarrages pneumatiques à action latérale - Série et modèles 2712-04X

Les amarrages pneumatiques à action latérale constituent une solution polyvalente pour un large éventail de matériaux. Capacités nominales comprises entre 1 et 10 kN.

Amarrages pneumatiques à action latérale - Séries 2712-05x

Les amarrages pneumatiques à action latérale constituent une solution polyvalente pour un large éventail de matériaux. Capacités nominales allant jusqu’à 250 N.

Série 2710 Amarrages à vis à action latérale

Les amarrages à vis à action latérale constituent une méthode très simple et efficace pour maintenir les échantillons d’essais et sont utilisables dans le cadre de nombreuses applications.