EN 12242 Peel Strength Touch and Close Fasteners (Hook and Loop)
- Textiles
- Tension
- Peel
- EN 12242
EN 12242 is a test method used to determine the peel strength of a touch and close (also known as “hook and loop”) fastener. A touch and close fastener is made up of two different types of materials: the male material is constructed with monofilament warp ends and finished to form-locking elements of either “hook” or “mushroom” shape. The female material is constructed with multifilament yarns in “loops”. When the two types of material are pressed together, the male and female elements engage to form a secure closure which can be separated by a peeling action from either end.
EN 12242 is widely used in the textile industry to evaluate different hook and loop fasteners. These fasteners have a wide range of uses, from apparel and footwear to consumer products to more industrial usage. In all cases, a complete understanding of their properties are important to ensure they perform as expected. The primary results of interest are minimum, maximum, and average peel strength.
Materials Testing SystemSystem capacity will depend on the strength of the fasteners. However, most tests to EN 12242 will fall in the 1 kN and 5 kN capacity range, making this application perfect for a single column frame such as Instron's 34SC or 68SC. Optimal gripping solutions include pneumatic side action and advanced side action grips, both of which feature quick-change jaw faces that can be easily changed to accommodate different materials as needed. Rubber-coated jaw faces are well suited to testing hook and loop fasteners.
EN 12242 Test Setup | |
---|---|
1) | 6800 Series Universal Testing System |
2) | Bluehill Universal Software |
3) | 2580 Series Load Cell |
4) | 2710 Series Advanced Side Action Grips |

For peel tests, it is critical to use a high data acquisition rate to capture all peaks and troughs to ensure all test events are fully represented in the results. Too low of a bandwidth may “dull” the results and lead to artificially low peel strength values. Instron’s 6800 series frames enable a data capture rate of up to 2.5kHz. With the Bluehill Universal Advanced Performance option, data acquisition rate can be increased to 5 kHz.
Série 6800 Brochure sur les systèmes d’essai de première qualité
Les systèmes d'essai universels Instron série 6800 offrent une précision et une fiabilité inégalées. Construit sur une architecture système Operator Protect en instance de brevet avec un tout nouveau kit de régulation d’air Smart-Close et des fonctions d’atténuation des collisions, la série 6800 rend les essais de matériaux plus simples, plus intelligents et plus sûrs que jamais.
Solutions d'essai abordables - Série 3400
Systèmes d'essai universels Instron série 3400 pour les essais de traction, de compression, de flexion et autres essais de propriété des matériaux.
Brochure de Bluehill Universal
Le logiciel Bluehill Universal est conçu dès le départ pour une interaction tactile et une expérience utilisateur intuitive. Vous découvrirez que les essais deviennent plus simples et plus intelligents grâce à des fonctionnalités, telles que les méthodes d’essais préconfigurées, le QuickTest fait en quelques secondes, l’exportation de données optimisée et Instron Connect - une nouvelle fonctionnalité qui fournit un lien de communication direct avec le service technique. Les utilisateurs des versions précédentes du logiciel, telles que Bluehill 2 et Bluehill 3, peuvent facilement faire la mise à jour à la toute dernière version de Bluehill.
Amarrages pneumatiques à action latérale - Série et modèles 2712-04X
Les amarrages pneumatiques à action latérale constituent une solution polyvalente pour un large éventail de matériaux. Capacités nominales comprises entre 1 et 10 kN.
Série 2710 Amarrages à vis à action latérale
Les amarrages à vis à action latérale constituent une méthode très simple et efficace pour maintenir les échantillons d’essais et sont utilisables dans le cadre de nombreuses applications.