EN 1465 Adhesives Lap Shear Bond Strength of Rigid-to-Rigid Assemblies
Written by Meredith Bernstein
- Adhesives
- Tension
- EN 1465
EN 1465 is a tensile test used to measure the adhesive lap-shear bond strength of rigid-to-rigid assemblies. This standard is used by many industries to test adhesives applied to materials such as metals, plastics, wood, and composites. Lap-shear strength is a critical characteristic of any adhesive, as they can exhibit unique shear properties.
EN 1465 is extremely similar to ISO 4587 with the exception of test rate. Both standards use identical test setups, specimen geometries, and results reporting, with the exception that ISO 4587 calls out a specific test rate of 8.3MPa to 9.8MPa while EN 1465 only specifies a constant rate of load application. Both standards state that the average specimen should break in a period of 65+/-20 sec.
Materials Testing SystemEN1465 is performed on a universal testing machine with a system capacity dependent on the strength of the adhesive. Most tests to this standard will fall into the capacity range between 1 kN and 5 kN, making this application perfect for a single column test frame such as Instron's 34SC or 68SC. If the adhesive requires a higher capacity system, Instron’s dual column table model frames are available up to 50 kN.

EN 1465 Test Setup
1. Instron 34SC-05
2. Bluehill Universal Dashboard (2490-696)
3. 2530 Series Load Cell (2530-100N)
4. 500 N Screw Side-Action Grips (2710-112)
Both pneumatic side-action grips and advanced screw side-action grips are excellent gripping choices for this standard. Both types of grips are adjustable in order to offset the jaw faces and ensure that the lap joint remains centered, and both feature quick-change jaw faces that can be easily changed to accommodate different materials.
- When testing lap shear specimens, the lap joint causes the two ends of the specimen to be offset from the vertical load line of the test. In order to ensure that the specimen remains centered in the load string and yields a true shear force calculation, the grips must have offset jaw faces to ensure they are directly aligned with the plane of the adhesive bond.
- EN 1465 requires reporting the breaking force or strength, however, it is important to remember that shear strength is calculated by dividing the breaking force by the adhesive bond area.
- Users who purchase Instron's Bluehill Universal software are provided with one free application module upon purchase. Each module contains pre-configured test methods and supporting documentation to assist with testing to various standards, including EN 1465 which is part of the Adhesives module.
Série 6800 Brochure sur les systèmes d’essai de première qualité
Les systèmes d'essai universels Instron série 6800 offrent une précision et une fiabilité inégalées. Construit sur une architecture système Operator Protect en instance de brevet avec un tout nouveau kit de régulation d’air Smart-Close et des fonctions d’atténuation des collisions, la série 6800 rend les essais de matériaux plus simples, plus intelligents et plus sûrs que jamais.
Solutions d'essai abordables - Série 3400
Systèmes d'essai universels Instron série 3400 pour les essais de traction, de compression, de flexion et autres essais de propriété des matériaux.
Brochure de Bluehill Universal
Le logiciel Bluehill Universal est conçu dès le départ pour une interaction tactile et une expérience utilisateur intuitive. Vous découvrirez que les essais deviennent plus simples et plus intelligents grâce à des fonctionnalités, telles que les méthodes d’essais préconfigurées, le QuickTest fait en quelques secondes, l’exportation de données optimisée et Instron Connect - une nouvelle fonctionnalité qui fournit un lien de communication direct avec le service technique. Les utilisateurs des versions précédentes du logiciel, telles que Bluehill 2 et Bluehill 3, peuvent facilement faire la mise à jour à la toute dernière version de Bluehill.
Amarrages pneumatiques à action latérale - Série et modèles 2712-04X
Les amarrages pneumatiques à action latérale constituent une solution polyvalente pour un large éventail de matériaux. Capacités nominales comprises entre 1 et 10 kN.
Série 2710 Amarrages à vis à action latérale
Les amarrages à vis à action latérale constituent une méthode très simple et efficace pour maintenir les échantillons d’essais et sont utilisables dans le cadre de nombreuses applications.