EN 868-5 characterizes the seal strength of single-use sterilized medical packaging. This standard specifically focuses on packaging materials and systems for medical devices which need to be sterilized. The seal strength identifies the adhesion strength between the two materials of the packaging; typically, a coated paper backing, and a plastic film overlay. This standard is technically equivalent to ASTM F88 with minor differences in the specimen preparation and test procedure.

While packaging can span many industries, The seal strength of medical packaging is extremely important for two reasons – first to ensure that the packing can be opened easily by the medical professional, and second to ensure that the adhesive is strong enough to prevent any breaches of the packaging prior to their use. During shipping and storage the adhesive must remain viable to maintain sterilization: any breach in the packaging would desterilize the product potentially leading to life threatening infections for the patient.

EN 868-5 Test Setup EN 868-5 can be performed on an Instron 3400 or 6800 Series single column universal testing system with a 500 N load cell.



EN 868-5 Test Setup
3400 Series Universal Testing System
Bluehill Universal Software
2530 Series Load Cell
2710-112 Screw Side Action Grips

 

EN 868-5 peel test of sterile medical packaging
Grips

When testing an adhesive to a thick substrate, standard grips result in a misaligned specimen. Testing to EN 868-5 requires either advanced screw side action grips or pneumatic side action grips, both of which can be adjusted to offset to ensure that the specimen remains centered in the load string. Pneumatic grips provide an advanced solution by ensuring a repeatable gripping force to eliminate slippage specimen slippage. Both options can be fitted with specimen centering devices to ensure proper alignment for each test, and both employ a patented “quick-change” jaw face design which enables operators to easily change jaw faces to accommodate the needs of their materials. Rubber-coated grip faces should be used so as to avoid tearing the delicate specimen. Jaw faces are available in many different sizes and are easily interchangeable. 

250 N Model | 2712-052
2710-112
500 N Model | 2710-112
Tips and Tricks

The specimen width and test speed are different than ASTM F88, but produce statistically similar results when the data is normalized.

Related Content

Brochure sur les systèmes d’essais de première qualité de la série 6800

Les systèmes d'essais universels Instron série 6800 offrent une précision et une fiabilité inégalées. Construit sur une architecture système Operator Protect en instance de brevet avec un tout nouveau kit de régulation d’air Smart-Close et des fonctions d’atténuation des collisions, la série 6800 rend les essais de matériaux plus simples, plus intelligents et plus sûrs que jamais.

Solutions d'essais abordables - Série 3400

Systèmes d'essais universels Instron série 3400 pour les essais de traction, de compression, de flexion et autres essais de propriété des matériaux.

Brochure Bluehill Universal

Le logiciel Bluehill Universal est intégralement conçu pour une interaction tactile et une expérience utilisateur intuitive. Vous découvrirez que les essais deviennent plus simples et plus intelligents grâce à des fonctionnalités, telles que les méthodes d’essais préconfigurées, le QuickTest fait en quelques secondes, l’exportation de données optimisée et Instron Connect - une nouvelle fonctionnalité qui fournit un lien de communication direct avec le service technique. Les utilisateurs des versions précédentes du logiciel, telles que Bluehill 2 et Bluehill 3, peuvent facilement faire la mise à jour à la toute dernière version de Bluehill.

Mors pneumatiques à action latérale - Série et modèles 2712-04X

Les mors pneumatiques à action latérale constituent une solution polyvalente pour un large éventail de matériaux. Capacités nominales comprises entre 1 et 10 kN.

Amarrages à vis à action latérale - Série 2710

Les amarrages à vis à action latérale constituent une méthode très simple et efficace pour maintenir les échantillons d’essais et sont utilisables dans le cadre de nombreuses applications.