For mounting ElectroPuls table-top systems when used for low to medium acceleration dynamic tests (accelerations below 6g)
Robust design with high stiffness grey frame and light-grey scratch-resistant table-top
Pre-drilled with mounting holes to suit E1000 or E3000 systems
Leggi di più ...
Robust design with high stiffness grey frame and light-grey scratch-resistant table-top
Pre-drilled with mounting holes to suit E1000 or E3000 systems
Model | Height | Width | Depth | Weight | ||||
---|---|---|---|---|---|---|---|---|
mm | in | mm | in | mm | in | kg | lb | |
1300-311 | 785 | 31 | 1000 | 39 | 750 | 30 | 56 | 123 |