ASTM F2516 Tensile Testing of Nitinol Wire

ASTM F2516 nitinol wire testing 

ASTM F2516 measures the tensile properties of superelastic nickel-titanium or Nitinol. The material properties of nitinol are different from those of most other materials – nitinol will change its structure depending on its temperature or the amount of stress applied to it. This means that it will exhibit very different stress strain profiles during loading and unloading, which is why this standard captures both an upper and lower plateau strength, rather than a singular yield strength. The ASTM F2516 test method is designed to pull the material in tension to 6% strain, then unload the material to a value of less than 7MPa before being pulling it to failure. 

What is Nitinol Used For? 

Nitinol's unique properties mean that it is used extensively in the biomedical industry to create stents, dental wires, catheter guidewires, internal fracture fixation devices, and biopsy forceps. One of its properties - shape memory - enables it to "remember" its shape when formed at a certain temperature. When the temperature is lowered beyond this point Nitinol can be molded to any other shape, but will automatically revert to its original shape once it reaches the temperature at which it was initially formed. This property makes it extremely useful for the creation of stents, which are used to hold open blood vessels and prevent severe clots. The stent can be transported through the body to the target location in a compacted form, reforming to its original cylindrical form once it warms up to body temperature at the target location. Nitinol is also commonly used for braces – the Nitinol is molded into the desired final shape, and the temperature within the mouth stresses the material to reform, slowly adjusting the teeth into their ideal positions. Unlike more traditional braces, nitinol braces wire is especially beneficial because it does not require frequent retightening.

Test Setup

ASTM F2516 is typically performed on a dual column materials testing system such as Instron's 6800 Series. A 5 kN load cell is most likely appropriate for most materials. Bluehill Universal software with TestProfiler is also required, and the test method for ASTM F2516 comes pre-loaded in Bluehill Universal's Biomedical Applications Module. 




ASTM F2516 Test Setup
1) 6800 Series Universal Testing System
2) Bluehill Universal Software
3) 2580 Series Load Cell
4) 2714-005 Pneumatic Cord and Yarn Grips

 

ASTM F2516 test setup nitinol wire
Grips and Fixtures

The gripping solution is dictated by specimen diameter, with most small diameters being tested with pneumatic cord and yarn grips and larger diameters utilizing pneumatic side action grips with serrated faces.

 

2712-041
1 kN Model | 2712-041
1 kN Model | 2714-005
Strain Measurement 

The diameter of the wire being tested determines the extensometry class required. For any wire 0.2 mm or smaller in diameter, crosshead movement can be used for strain measurement. Diameters greater than 0.2mm require a class C extensometer, with Instron's AUTOX automatic contacting extensometer, and AVE2 non-contacting extensometers being popular choices, as the weight of clip-on devices can affect results when testing such small specimens.

Specimen diameter and gauge length also determine test speed, so utilizing expression builder in Bluehill Universal can provide an easy way to update the test speed automatically. The lab temperature for this test is also very important - the material needs to be tested at a temperature at least 5 degrees higher than its austenitic finish transformation temperature. If not, the material will be partially transformed to a different material state, affecting the results.

Related Content

6800 Opuscolo sui sistemi di test Premier della serie

I sistemi di test universali della serie 6800 di Instron offrono precisione e affidabilità impareggiabili. Grazie alla serie 6800, costruita sulla base di un’architettura di sistema in attesa di brevetto e dotata delle nuovissime funzionalità Smart-Close Air Kit e Collision Mitigation, i test dei materiali non sono mai stati così semplici, intelligenti e sicuri.

Serie 3400 - Soluzioni per test convenienti

Sistemi di test universali della serie 3400 Instron per test di trazione, compressione, piegatura e altri test di proprietà dei materiali.

Opuscolo su Bluehill Universal

Bluehill Universal Software è realizzato appositamente per l’interazione touch e un’esperienza utente intuitiva. Scopri test più semplici e più intelligenti con funzionalità quali i metodi di test precaricati, QuickTest in pochi secondi, esportazione di dati migliorata e Instron Connect, una nuova caratteristica che fornisce un collegamento diretto di comunicazione con l’Assistenza. Gli utenti delle versioni precedenti del software come Bluehill 2 e Bluehill 3 possono facilmente aggiornarle alla versione più recente di Bluehill.

TestProfiler per Bluehill Universal

La funzionalità TestProfiler di Bluehill Universal’ offre una flessibilità senza precedenti nella progettazione di test che automatizzano una sequenza di passaggi.

Prese pneumatiche ad azione laterale serie 2712-04x

Le prese pneumatiche ad azione laterale forniscono una soluzione versatile per la presa di una vasta gamma di materiali. Capacità nominali tra 1 e 10 kN.

Prese di trazione pneumatiche per corde e filati 2714-005

Le prese di trazione pneumatiche per corde e filati forniscono un metodo conveniente per il serraggio di fibre, corde, filati e fili sottili per ridurre il problema associato al test di questi materiali. Capacità nominale 1 kN.

AVE 2 Estensimetro video senza contatto

La seconda generazione dell’estensimetro video avanzato (Advanced Video Extensometer, AVE 2) utilizza una tecnologia di misurazione brevettata nel dispositivo di misurazione della deformazione senza contatto più veloce e precisa disponibile sul mercato.

Estensimetro a contatto automatico, modello AutoX 750

L’AutoX 750 è un estensimetro a contatto automatico ad alta risoluzione e a lunga corsa. Può essere montato su qualsiasi sistema elettromeccanico 3300, 3400, 5500, 5900, o 6800 da tavolo e a pavimento, così come sui sistemi di test idraulico statico LX, DX, HDX e KPX. È adatto per applicazioni che coinvolgano materie plastiche, metalli, biomedicale, compositi, elastomeri e altro. L’AutoX ha una corsa massima di 750 mm e una precisione di ± 1 µm.