ASTM D1414 Standard Test Methods for Rubber O-Rings
- Elastomers
- Tension
- ASTM 1414
ASTM D1414 specifies the procedures for determining the physical properties of o-rings. O-rings are typically made of elastomeric material and are used to seal connections in pipes, tubes, etc. This testing standard is commonly used in the safety-critical aerospace, automotive, and consumer products industries.
Materials Testing SystemThough system capacity will depend on the strength of the elastomer, most tests to this standard will fall in the low-force range, making this application perfect for a single column frame such as Instron's 68SC or 34SC. The standard specifies a fixture consisting of two spools to hold an o-ring while under test. Instron’s 2717 Series elastomeric o-ring test fixtures were designed to accurately meet the requirements, and conveniently avoid the need for lubricants or external power motors. Designed for testing elastomeric materials in the form of rings, these fixtures avoid local stress concentrations by using a lower spindle that is rotated by a toothed belt driven from the moving crosshead. The upper spindle rotates freely, and the rotation frequency of the lower spindle is easily selected by moving the toothed belt from one pulley to another. When testing straight specimens or single strands, pneumatic side action grips with serrated or rubber coated faces are the preferred gripping configuration. The constant gripping force prevents specimen slippage while under test.
ASTM D1414 Test Setup | |
---|---|
1) | 6800 Series Universal Testing System |
2) | Bluehill Universal Software |
3) | 2580 Series Load Cell |
4) | 2717 Series O-Ring Fixture |

- Due to the geometry of o-rings and the unique fixture needed to test them, standard stress (F/A) and strain calculations (∆L/Lo) do not apply. Consideration needs to be made for the fixture geometry (spool separation and diameter) as well as specimen geometry.
- Bluehill Universal is provided with one free application module upon purchase. Each module contains pre-configured test methods and supporting documentation to assist with testing to various standards, including ASTM D1414, which is part of the Elastomers module.
- The Expression Builder within Bluehill Universal software allows for custom calculations and results in order to adhere to the standard.
- To review the test methods in full, purchase ASTM D1414.
6800 Opuscolo sui sistemi di test Premier della serie
I sistemi di test universali della serie 6800 di Instron offrono precisione e affidabilità impareggiabili. Grazie alla serie 6800, costruita sulla base di un’architettura di sistema in attesa di brevetto e dotata delle nuovissime funzionalità Smart-Close Air Kit e Collision Mitigation, i test dei materiali non sono mai stati così semplici, intelligenti e sicuri.
Serie 3400 - Soluzioni per test convenienti
Sistemi di test universali della serie 3400 Instron per test di trazione, compressione, piegatura e altri test di proprietà dei materiali.
Opuscolo su Bluehill Universal
Bluehill Universal Software è realizzato appositamente per l’interazione touch e un’esperienza utente intuitiva. Scopri test più semplici e più intelligenti con funzionalità quali i metodi di test precaricati, QuickTest in pochi secondi, esportazione di dati migliorata e Instron Connect, una nuova caratteristica che fornisce un collegamento diretto di comunicazione con l’Assistenza. Gli utenti delle versioni precedenti del software come Bluehill 2 e Bluehill 3 possono facilmente aggiornarle alla versione più recente di Bluehill.
Prese pneumatiche ad azione laterale serie 2712-04x
Le prese pneumatiche ad azione laterale forniscono una soluzione versatile per la presa di una vasta gamma di materiali. Capacità nominali tra 1 e 10 kN.