ASTM D1621 Compressive Properties Rigid Cellular Plastics

ASTM D1621 testing

plastics hub icon 

ASTM D1621 outlines the testing procedure for determining the compressive properties of rigid cellular materials, particularly expanded plastics. Rigid cellular, or foamed, plastics are manufactured in different forms for a variety of construction-related applications. Properties common to cellular plastic include thermal insulation (heat loss or fire protection), sound absorption, high strength-to-weight ratio, and earthquake resistance. The properties possessed by any given cellular plastic are a product of its resin, its cellular structure (open vs. closed), and its density. Material properties reported during ASTM D1621 testing include compression strength, strain at compressive strength, yield points, and if requested, compressive modulus.

 

Testing System

Depending on the maximum expected forces, ASTM D695 can be performed on either a single column or dual column universal testing machine such as those available in Instron's 6800 and 3400 Series.


ASTM D1621 Test Setup
3400 Series Universal Testing System
Bluehill Universal Software
2530 Series Load Cell
2501 Series Compression Platens

 

ASTM D1621 test setup
Platens and Accessories

The preferred specimen dimensions for ASTM D1621 testing are a square or circular cross-sectional area between 4 and 36 square inches and a height between 1 inch and the specimen’s width (or diameter). Note the dimensional differences between a D1621 and D695 specimen, which are both ATSM compression test standards for plastic materials. Compression platens with integral spherical seats are ideal for ensuring platen to platen parallelism, which is a requirement of the standard. Depending on your application, the following are commonly used for ASTM D1621 testing:




ASTM D1621 Accessories
Self-Aligning Spherical Seat
2601-04x Series LVDT

 

ASTM D1621
Helpful Tips and Tricks
  • Compression platens with integral spherical seats are ideal for ensuring platen to platen parallelism, which is a requirement of the standard. The self-aligning nature of this fixture will maximize the contact area between the platen and the specimen.
  • When measuring compressive displacement, ASTM D1621-16 allows for measurement using direct compression platen displacement or via crosshead extension by eliminating the effects of system compliance. If direct strain measurement is used, a displacement transducer is required to measure the distance between the upper and lower platen. The transducer must also be verified in conformance with ASTM E83 Class C or better. Instron's 2601-04x series LVDTs can mount directly on the 2501 series compression platens and are designed to measure displacement directly from the platens. To measure displacement via crosshead extension, Bluehill Universal testing software can do an automatic compliance correction to eliminate system compliance from the test curve. Please review the compliance correction whitepaper for more details. 
  • If reporting the modulus calculation, make sure the extensometer and load cell are both verified in the range that the calculation is being made. Labs sometimes unknowingly report calculations outside of the verified range of their devices.
  • It is important to review ASTM D1621-16 in order to fully understand the test setup, procedure, and results requirements.
Related Content

Serie 6800 - Opuscolo dei sistemi di test Premier

I sistemi di test universali della serie 6800 di Instron offrono precisione e affidabilità impareggiabili. Grazie alla serie 6800, costruita sulla base di un’architettura di sistema in attesa di brevetto e dotata delle nuovissime funzionalità Smart-Close Air Kit e Collision Mitigation, i test dei materiali non sono mai stati così semplici, intelligenti e sicuri.

Serie 3400 - Soluzioni per test convenienti

Sistemi di test universali della serie 3400 Instron per test di trazione, compressione, piegatura e altri test di proprietà dei materiali.

Opuscolo su Bluehill Universal

Bluehill Universal Software è realizzato appositamente per l’interazione touch e un’esperienza utente intuitiva. Scopri test più semplici e più intelligenti con funzionalità quali i metodi di test precaricati, QuickTest in pochi secondi, esportazione di dati migliorata e Instron Connect, una nuova caratteristica che fornisce un collegamento diretto di comunicazione con l’Assistenza. Gli utenti delle versioni precedenti del software come Bluehill 2 e Bluehill 3 possono facilmente aggiornarle alla versione più recente di Bluehill.

Piani di compressione con sede sferica serie S571x

Facili da installare, questi piani di compressione sono attrezzature lavorate con precisione e progettate per una distribuzione uniforme dei carichi di compressione durante un test. La stringa di carico di compressione comprendente un piano superiore con sede sferica integrale e una piastra rigida inferiore è fissata all’asse di caricamento della macchina di prova universale.

Piani di compressione serie 2501

Facili da installare, questi piani di compressione sono attrezzature lavorate con precisione e progettate per una distribuzione uniforme dei carichi di compressione durante un test.

Sensori di deformazione LVDT serie 2601

I trasduttori di spostamento del trasformatore differenziale lineare (LVDT) della serie 2601 sono dispositivi che misurano lo spostamento dei telai di carico.