ASTM D575-91: Standard Test Methods for Rubber Properties in Compression
- Elastomers
- Compression
- ASTM D575
ASTM D575 is a testing standard used to determine the stiffness of rubber materials in compression. ASTM D575 allows rubber suppliers to characterize the stiffness of the material they produce to help downstream manufacturers source the correct material for their components. Data collected from ASTM D575 testing is important for applications that require elastomeric materials subjected to compressive stresses. One wide-ranging application is the sealant industry, as due to its ease of extrusion and flexible nature, rubber is commonly used material for sealants.
Method A applies a predetermined deflection to the cylindrical specimen at which the force is recorded. Alternatively, Method B applies predetermined minor and major forces to the specimen and deflection is measured.
Materials Testing SystemDepending on maximum expected forces, ASTM D575 is performed on a single column or dual column universal testing system such as Instron's 3400 and 6800 Series systems. This system setup requires a matching load cell and upper and lower platens with diameters larger than the diameter of the specimen. Platens should have rigid connections to the frame and load cell, and must be rated to a load capacity which exceeds forces generated during the test.ASTM D575 Test Setup | |
---|---|
1) | 3400 Series Universal Testing System |
2) | Bluehill Universal Software |
3) | 2530 Series Load Cell |
4) | 2501 Series Compression Platens |

Though not required by the standard, parallelism can be ensured by including an integral spherical seat on the upper platen. Though crosshead displacement measurements are adequate for ASTM D575, those interested in the most accurate deflection measurement should consider using a 2601-04x Series linear variable displacement transducer.
ASTM D575 Accessories | |
---|---|
1) | Self-Aligning Spherical Seat |
2) | 2601-04x Series LVDT |

- For the most accurate deflection measurements, we recommend a 2601 series LVDT attached to the platen itself over the use of crosshead displacement measurement. If crosshead position is used, it is important to use Corrected Displacement in Bluehill Universal to prevent error from machine compliance.
- Is parallelism of platens important to your lab? If so, compression platens with integral spherical seats are ideal for ensuring platen to platen parallelism.
- If performing ASTM D575 Method B with an Instron machine, be aware that a force hold is a requirement of the test. Similar to longer creep or stress-relaxation tests, holding force requires the load cell’s transducer settings to be tuned to the effective stiffness of test setup, which includes the specimen itself and any fixturing.
6800 Opuscolo sui sistemi di test Premier della serie
I sistemi di test universali della serie 6800 di Instron offrono precisione e affidabilità impareggiabili. Grazie alla serie 6800, costruita sulla base di un’architettura di sistema in attesa di brevetto e dotata delle nuovissime funzionalità Smart-Close Air Kit e Collision Mitigation, i test dei materiali non sono mai stati così semplici, intelligenti e sicuri.
Serie 3400 - Soluzioni per test convenienti
Sistemi di test universali della serie 3400 Instron per test di trazione, compressione, piegatura e altri test di proprietà dei materiali.
Opuscolo su Bluehill Universal
Bluehill Universal Software è realizzato appositamente per l’interazione touch e un’esperienza utente intuitiva. Scopri test più semplici e più intelligenti con funzionalità quali i metodi di test precaricati, QuickTest in pochi secondi, esportazione di dati migliorata e Instron Connect, una nuova caratteristica che fornisce un collegamento diretto di comunicazione con l’Assistenza. Gli utenti delle versioni precedenti del software come Bluehill 2 e Bluehill 3 possono facilmente aggiornarle alla versione più recente di Bluehill.
Piani di compressione serie 2501
Facili da installare, questi piani di compressione sono attrezzature lavorate con precisione e progettate per una distribuzione uniforme dei carichi di compressione durante un test.
Sensori di deformazione LVDT serie 2601