ASTM D5766 Open-Hole Tensile Strength of Polymer Matrix Composite Laminates

ASTM D5766 open-hole tensile strength of polymer matrix composite laminates

ASTM D5766 determines the open-hole tensile strength of multidirectional composite coupons. The composite coupon geometry has to be in accordance with test method ASTM D3039. ASTM D5766 is designed to produce tensile results on multidirectional polymer matrix composite laminates mainly used in the aerospace industry for material specifications, research and development, quality assurance, and structural design and analysis.

Materials Testing System

Because the forces required for ASTM D5766 testing are relatively high, a floor model universal testing system such as Instron's 6800 Series is recommended. The properties of composite materials are highly directional, making it especially necessary to test with a system that is well-aligned and repeatable. An AlignPRO fixture and precision manual or hydraulic wedge grips are necessary in order to test specimens within alignment requirements and without slippage.




ASTM D6484 Test Setup
6800 Series
Bluehill Universal Software
 2580 Series Load Cell
2742 Series Hydraulic Wedge Grips
AlignPro

 

ASTM D5766 composite testing system
Testing Tips and Tricks
  • This testing is performed in accordance with ASTM D3039, but instead of a uniform coupon, the specimen is modified with a centrally-located hole. When calculating the ultimate tensile strength based on the cross sectional area, the hole's presence is disregarded.
  • ASTM D5766 requires that the specimen coupon have multidirectional fiber orientations in a minimum of two directions. Typical test results include the ultimate tensile strength, the width of specimen-to-hole diameter ratio, hole-diameter-to-coupon-thickness ratio, and, if desired, the edgewise percent bending in accordance with ASTM D3039.
  • The only valid failure mode in determining the ultimate tensile strength is one that passes through the prefabricated hole in the test coupon. A break outside of this location does not deliver valid test results.
  • To learn more, purchase ASTM D5766
Related Content

Opuscolo sui test dei materiali compositi

Le macchine di prova universali di Instron sono progettate per eseguire i tipi di test più comuni nel settore dei compositi tra cui, a titolo esemplificativo ma non esaustivo, la trazione sul piano, la trazione a spessore variabile, il taglio interlaminare, la compressione finale, il taglio o il carico combinato e la compressione post impatto.

Opuscolo sulle macchine di prova universali ad alta forza

I sistemi ad alta forza di Instron includono sistemi di test elettromeccanici e idraulici ad alta capacità per applicazioni di tensione e compressione. Le capacità di forza vanno da 100 kN a 2000 kN.

Sistema di allineamento AlignPRO

Il sistema AlignPRO™ di Instron è progettato per assistere gli operatori nella misurazione e nella regolazione dell’allineamento della stringa di carico.

2743-401 - Prese idrauliche con azione a cuneo

Le prese idrauliche con azione a cuneo da 100 kN di Instron offrono una soluzione innovativa per test ad alta capacità e per fornire prestazioni di presa migliorate, facilità d’uso e sicurezza dell’operatore.

2716 Prese manuali di precisione con azione a cuneo

Disponibili con capacità da 100 e 250 kN, le prese manuali di precisione con azione a cuneo 2716-028/30 di Instron offrono una presa affidabile per un’ampia gamma di materiali e un allineamento ripetibile conforme ai requisiti Nadcap.