ASTM D5961 - Bearing Response of Polymer Matrix Composite Laminates

ASTM D5961 Bearing Response of Polymer Matrix Composite Laminates

ASTM D5961 is a testing standard that covers the bearing response of pinned or fastened joints of composite laminates. Connecting individual composite components with rivets or fastener is a common solution for connection of parts in the aerospace industry. ASTM D5961 is used by material designers to determine material specifications for research and development, quality assurance, and structural design analysis.

Test Methods

ASTM D5961 includes four different testing procedures: A, B, C, and D. Procedure A is designed for double-shear tensile loading on a single piece specimen. Procedure B is for single-shear tensile or compressive loading on a two piece specimen. Procedure C is for single shear tensile loading of a single piece specimen, and Procedure D is for double-shear compressive loading on a single piece coupon. The composite coupons are supposed to be balanced and symmetric with respect to their test direction. 

It is important to note that these four testing procedures will give results that are not directly comparable. Due to the larger fastener rotation and higher peak bearing stress Procedure C will yield higher strengths than Procedure B. For protruding head fasteners Procedure D will most likely yield higher bearing results than Procedure C. Procedures A and C produce very similar results.

Materials Testing System

ASTM D5961 testing is best performed on a high capacity system such as Instron's 100kN 6800 Series floor model equipped with either precision manual (2716-028/030) or hydraulic (2743-401)wedge grips for gripping the loading plates. This standard requires different loading tools for each procedure, usually involving loading plates, pins, and/or fasteners. A set of grips is needed to grip the loading plates.

For more information, download ASTM D5961


ASTM D5961 Test Setup
6800 Series universal testing system
Bluehill Universal software
2580 Series load cell
 2743 Series hydraulic wedge grip

 

ASTM D5961 test setup
Related Content

Opuscolo sui test dei materiali compositi

Le macchine di prova universali di Instron sono progettate per eseguire i tipi di test più comuni nel settore dei compositi tra cui, a titolo esemplificativo ma non esaustivo, la trazione sul piano, la trazione a spessore variabile, il taglio interlaminare, la compressione finale, il taglio o il carico combinato e la compressione post impatto.

Opuscolo sulle macchine di prova universali ad alta forza

I sistemi ad alta forza di Instron includono sistemi di test elettromeccanici e idraulici ad alta capacità per applicazioni di tensione e compressione. Le capacità di forza vanno da 100 kN a 2000 kN.

2716 Prese manuali di precisione con azione a cuneo

Disponibili con capacità da 100 e 250 kN, le prese manuali di precisione con azione a cuneo 2716-028/30 di Instron offrono una presa affidabile per un’ampia gamma di materiali e un allineamento ripetibile conforme ai requisiti Nadcap.

Opuscolo su Bluehill Universal

Bluehill Universal Software è realizzato appositamente per l’interazione touch e un’esperienza utente intuitiva. Scopri test più semplici e più intelligenti con funzionalità quali i metodi di test precaricati, QuickTest in pochi secondi, esportazione di dati migliorata e Instron Connect, una nuova caratteristica che fornisce un collegamento diretto di comunicazione con l’Assistenza. Gli utenti delle versioni precedenti del software come Bluehill 2 e Bluehill 3 possono facilmente aggiornarle alla versione più recente di Bluehill.