ASTM E290 Bend Testing of Material for Ductility
- Metals
- Flexure
- ASTM E290
ASTM E290 describes the testing requirements used to determine the ductility of metals through bend testing. Bend testing helps provide a visual indication of the material's ductility. ASTM E290 is divided into four methods for bending the specimen:
- Guided Bend
- Semi-Guided Bend
- Free-Bend
- Bend and Flatten.
These tests are performed by supporting the two ends of a specimen while loading it at the center with a mandrel or plunger. The test is completed when the designated angle of the bend, or other specified condition, has been reached. Afterwards, the specimen is visually inspected for cracks or defects, and failure is determined by the size of the cracks and imperfections allowed by the material specification.
Materials Testing SystemFor ASTM E290 testing we recommend using an Industrial Series DX or HDX model with Bluehill Universal software and a W-6810 test fixture. This fixture allows for adjustment of the support span and is supplied with various sizes of loading mandrels to accommodate different specimen thicknesses. The loading supports are held together with two tie rods to provide extra stiffness during loading. The DX or HDX Model dual test space load frames allow the bend test fixture to be positioned in the lower compression test space. Any tensile testing can also be accomplished in the upper tensile test space.
ASTM E290 Test Setup | |
---|---|
1) | Instron 1000 HDX |
2) | W-5340 Hydraulic Wedge Action Grips |
3) | W-6810 test fixture |

Opuscolo sulle macchine di prova universali ad alta forza
I sistemi ad alta forza di Instron includono sistemi di test elettromeccanici e idraulici ad alta capacità per applicazioni di tensione e compressione. Le capacità di forza vanno da 100 kN a 2000 kN.
Modelli HDX della serie industriale
Con uno spazio di test doppio e un lungo stroke test, questi telai idraulici sono disponibili con capacità di 1.000 kN (225.000 lbf) e 1.500 kN (337.500 lbf).
Opuscolo su Bluehill Universal
Bluehill Universal Software è realizzato appositamente per l’interazione touch e un’esperienza utente intuitiva. Scopri test più semplici e più intelligenti con funzionalità quali i metodi di test precaricati, QuickTest in pochi secondi, esportazione di dati migliorata e Instron Connect, una nuova caratteristica che fornisce un collegamento diretto di comunicazione con l’Assistenza. Gli utenti delle versioni precedenti del software come Bluehill 2 e Bluehill 3 possono facilmente aggiornarle alla versione più recente di Bluehill.