EN 12242 Peel Strength Touch and Close Fasteners (Hook and Loop)

EN 12242 peel strength of touch and close fastners (hook and loop)

EN 12242 is a test method used to determine the peel strength of a touch and close (also known as “hook and loop”) fastener. A touch and close fastener is made up of two different types of materials: the male material is constructed with monofilament warp ends and finished to form-locking elements of either “hook” or “mushroom” shape. The female material is constructed with multifilament yarns in “loops”. When the two types of material are pressed together, the male and female elements engage to form a secure closure which can be separated by a peeling action from either end.

EN 12242 is widely used in the textile industry to evaluate different hook and loop fasteners. These fasteners have a wide range of uses, from apparel and footwear to consumer products to more industrial usage. In all cases, a complete understanding of their properties are important to ensure they perform as expected. The primary results of interest are minimum, maximum, and average peel strength.

Materials Testing System

System capacity will depend on the strength of the fasteners. However, most tests to EN 12242 will fall in the 1 kN and 5 kN capacity range, making this application perfect for a single column frame such as Instron's 34SC or 68SC. Optimal gripping solutions include pneumatic side action and advanced side action grips, both of which feature quick-change jaw faces that can be easily changed to accommodate different materials as needed. Rubber-coated jaw faces are well suited to testing hook and loop fasteners.




EN 12242 Test Setup
1) 6800 Series Universal Testing System
2) Bluehill Universal Software
3) 2580 Series Load Cell
4) 2710 Series Advanced Side Action Grips

 

EN 12242 system setup
Tips and Tricks

For peel tests, it is critical to use a high data acquisition rate to capture all peaks and troughs to ensure all test events are fully represented in the results. Too low of a bandwidth may “dull” the results and lead to artificially low peel strength values. Instron’s 6800 series frames enable a data capture rate of up to 2.5kHz. With the Bluehill Universal Advanced Performance option, data acquisition rate can be increased to 5 kHz.

6800 Opuscolo sui sistemi di test Premier della serie

I sistemi di test universali della serie 6800 di Instron offrono precisione e affidabilità impareggiabili. Grazie alla serie 6800, costruita sulla base di un’architettura di sistema in attesa di brevetto e dotata delle nuovissime funzionalità Smart-Close Air Kit e Collision Mitigation, i test dei materiali non sono mai stati così semplici, intelligenti e sicuri.

Serie 3400 - Soluzioni per test convenienti

Sistemi di test universali della serie 3400 Instron per test di trazione, compressione, piegatura e altri test di proprietà dei materiali.

Opuscolo su Bluehill Universal

Bluehill Universal Software è realizzato appositamente per l’interazione touch e un’esperienza utente intuitiva. Scopri test più semplici e più intelligenti con funzionalità quali i metodi di test precaricati, QuickTest in pochi secondi, esportazione di dati migliorata e Instron Connect, una nuova caratteristica che fornisce un collegamento diretto di comunicazione con l’Assistenza. Gli utenti delle versioni precedenti del software come Bluehill 2 e Bluehill 3 possono facilmente aggiornarle alla versione più recente di Bluehill.

Prese pneumatiche ad azione laterale serie 2712-04x

Le prese pneumatiche ad azione laterale forniscono una soluzione versatile per la presa di una vasta gamma di materiali. Capacità nominali tra 1 e 10 kN.

Serie 2710 Prese a vite ad azione laterale

Le prese a vite ad azione laterale forniscono un metodo molto semplice ed efficiente per tenere i provini di test e possono essere utilizzate in una vasta gamma di applicazioni.