EN 2597 Carbon Fiber Reinforced Plastics. Unidirectional Laminates. Tensile Test Perpendicular to the Fiber Direction

composites test and airplane

 

EN 2597:1998 is a testing standard that specifies the method of determination of the ultimate tensile strength, tensile modulusPoisson’s ratio, and strain at failure in tension of carbon fiber reinforced plastics in the form of unidirectional laminates. EN 2598 is used for product development and quality control by a range of manufacturers who use carbon fiber laminates, including the aerospace, automotive, wind energy, and construction industries. This method is only applicable to specimens where the axis is perpendicular to the direction of the fibers. Testing when the axis is parallel to the fiber direction calls for the use of EN 2561.

Materials Testing System

The strength of composite specimens with fibers oriented perpendicular to the loading direction (axis) are normally much lower than the strengths of specimens where the fibers are oriented in the loading direction. Hence, the test forces are much lower. However, since testing to EN 2597 is normally combined with a range of other, higher force tests on composite materials, an electromechanical floor model testing machine such as Instron's 6800 Series will be the most suitable solution. The large (1000:1) force measurement range of the 5980 means that both high and low force tests can be carried out without the need to change load cells. A table model electromechanical machine may have sufficient capacity for testing lower strength materials, such as glass fiber.




EN 2597 Test Setup
6800 Series Universal Testing System
Bluehill Universal Software
2580 Series Load Cell
2742 Series Hydraulic Wedge Grips
AVE2 Non-Contacting Extensometer

 

EN 2597 test system
Grips

Moving body grips meet the requirements of the standard and are available in both manually and hydraulically operated configurations. 


Catalog no. 2743-401

Catalog no. 2716-002



EN 2597 Testing Accessories
Strain Gauge
Biaxial Clip-On Extensometer
Environmental Chamber
Testing Accessories

Strain measurement devices include strain gauges and extensometers. Strain gauges can be connected to the testing machine via easy-to-use strain gauge adapters. A range of suitable contacting extensometers for axial and bi-axial strain measurements are available. When strain at failure is required, a non-contacting strain measurement solution such as Instron's AVE2 is preferred. When tests need to be conducted at high or low temperatures, a temperature chamber along with grips capable of operation inside the chamber are required. 


composites testing accessories

Testing Tips and Tricks
  • Obtaining consistent results when testing composites requires accurate alignment of the test specimen. Instron testing frames and accessories provide excellent alignment.
  • Bluehill Universal software comes provided with one free applications module upon purchase. The composites module includes a pre-defined EN 2597 test method.
  • To read the test method in full, purchase EN 2597:1998
Related Content

Opuscolo su Bluehill Universal

Bluehill Universal Software è realizzato appositamente per l’interazione touch e un’esperienza utente intuitiva. Scopri test più semplici e più intelligenti con funzionalità quali i metodi di test precaricati, QuickTest in pochi secondi, esportazione di dati migliorata e Instron Connect, una nuova caratteristica che fornisce un collegamento diretto di comunicazione con l’Assistenza. Gli utenti delle versioni precedenti del software come Bluehill 2 e Bluehill 3 possono facilmente aggiornarle alla versione più recente di Bluehill.

Opuscolo sui test dei materiali compositi

Le macchine di prova universali di Instron sono progettate per eseguire i tipi di test più comuni nel settore dei compositi tra cui, a titolo esemplificativo ma non esaustivo, la trazione sul piano, la trazione a spessore variabile, il taglio interlaminare, la compressione finale, il taglio o il carico combinato e la compressione post impatto.

AVE 2 Estensimetro video senza contatto

La seconda generazione dell’estensimetro video avanzato (Advanced Video Extensometer, AVE 2) utilizza una tecnologia di misurazione brevettata nel dispositivo di misurazione della deformazione senza contatto più veloce e precisa disponibile sul mercato.

Estensimetri per estensimetri serie 2630

La serie 2630-100 di estensimetri offre velocità di attacco e facilità d’uso. Il design leggero e robusto delle traverse elimina gli errori causati dalla deformazione fisica, mentre la protezione integrata assicura che i danni non siano causati da un’eccessiva estensione.

Estensimetri a clip assiali, biassiali e per misurazione media

Gli estensimetri a clip assiali, biassiali e per misurazione media di Instron utilizzano estensimetri a fini di misurazione e sono realizzati in alluminio ad alta resistenza, titanio e acciaio inossidabile.

Camere ambientali serie 3119-600

La camera ambientale serie 3119-600 consente ai laboratori di eseguire test sicuri ed efficienti a una vasta gamma di temperature non ambientali.

Adattatori per estensimetro

Gli estensimetri vengono utilizzati in diversi settori, dal quello aerospaziale a quello edile, per misurare la deformazione sia nei materiali, sia nei test strutturali. Questi adattatori per estensimetri consentono di utilizzare un singolo estensimetro con qualsiasi canale di deformazione Instron standard.