Thermoset and Thermoplastic Composites ... What’s the Difference?

As composites continue to be adopted in more industries, fiber-reinforced plastics can be found in products that people interact with every day, including cars and sporting goods. Fiber-reinforced plastics consist of reinforcing fibers surrounded by a plastic matrix. There are several types of fibers that can be used including glass, carbon fiber, and aramid which give the material its high tensile strength. The matrix gives the composite the compressive strength and, in the case of fiber reinforced plastics, can be made using thermoset or thermoplastic polymers.