A Case for Extensometry

A universal testing system very simply measures 2 things during a basic mechanical test: force (via the load cell) and displacement (via the crosshead encoder). To obtain a basic stress-strain curve, you might think that’s all you need. With the force measurement from the load cell, the cross-sectional area of the material can be used to calculate stress; and with the crosshead extension, the original distance between the grips or fixtures can be used to calculate strain throughout the test. How simple!

Posted By Elena Mangano

 Nov 05, 2014

blog

Question From a Customer: Air Bubbles in Extrudate

Q: We have an MF30 Melt Flow Indexer and started running tests on various polymers in our lab. Some of the samples have a lot of air bubbles in them. I believe this is contributing to inconsistencies in melt flow values. How do we minimize this? A: There are a lot of reasons you could be seeing air bubbles in the filament sample. Ultimately, it comes down to keeping the testing and cleaning processes as consistent as possible.