インストロン主催の新しいインストロン・コミュニティ・ブログへようこそ。 インストロンならではの最高にフレッシュかつ頭脳明晰で才能豊かな人々の集まりです。 材料科学の世界は果てしなく広く、膨大な業界や材料、課題が対象となっています。そのため、その道の専門家、あるいは材料科学の達人になるために必要なあらゆる知識を1人で備えるのは到底無理です。 コミュニティ・ブログには、専門的ノウハウや体験、アイデアを連携して出し合い、最も正確で関連のある情報をタイミング良く読者に提供してくれる豊富な人材が集まっています。

自己紹介、意見、そして自身の体験についてお話しください。 インストロン・コミュニティでお待ちしています。

Reducing Variablity in Plastics Testing

Although you may be testing to specifications that would allow you to comply with international standards, many factors can cause variability in your plastics testing results. The following presentation provides a summary of the most common explanations for test data variability, including specimen alignment and method setup:

Posted On Jun 23, 2014 02:10 PM

Instron Awarded by the United Way

We are proud to announce that our Community Connection Committee (C3) has been awarded the Campaign Coordinator Award for the fourth year in a row by the United Way of Tri-County. This honor is in recognition of a successful 2013 United Way Campaign to advance the local community through service and support.

Posted On Jun 22, 2014 02:10 PM

Webinar Archive Hosts Recordings

Instron live webinars provide the opportunity to hear updates from experts on industry news and testing techniques. If you happen to miss the webinars, our library hosts the recordings.



Posted On Jun 13, 2014 02:10 PM

Reminder to Not Let Your Standards Slip

You most likely understand the importance of regularly calibrating your testing and measuring equipment and making sure it is maintained to the highest standards to ensure the data that you capture is as accurate as possible. But do you regularly review your testing standards?

Posted On Jun 10, 2014 02:10 PM

Backward Strain at Yield — Discontinuous Yielding/YPE Material

During a recent customer visit, a concern was raised about a turnaround point on the graph that they had not previously seen. Following a bit of investigation, the customer was producing galvanized steel of various grades, some of which was aged. The graph below shows a magnified view of the fairly aggressive upper yield point (UYS or ReH), which results in an almost immediate drop in stress.

Posted By David Fry On  Jun 10, 2014 02:10 PM

Sorting Over 15,000 lbs. of Food Donations? No problem.

Instron employees volunteered to organize over 15,000 lbs. of food donations, gathered with the help of the United States Postal Service Stamp-Out-Hunger Food Drive. After the rewarding work, the team was all smiles.

Posted On Jun 10, 2014 02:10 PM

Instron's European Sales Director Discusses Rental Program

Tom Davies, European Sales Director, talks with AZoM about our contract rental program, piloted in the United Kingdom. The program offers the flexibility to rent Instron systems and accessories with no upfront investment. A rental can be issued on a monthly or a quarterly basis in order to try the latest equipment.

Posted On Jun 09, 2014 02:10 PM