Cleavage Test Fixture
S1-11860 | Cleavage Test Fixture
Wood Test Fixture.
Cleavage Tool per ASTM D143.
Upper and lower fittings: Type Dm (1.25 in connection with 1/2 in clevis pin).
アクセサリ重量 | 0.75 kg (1.65 lb) |
---|---|
アクセサリ幅 | 38 mm (1.5 in) |
荷重容量 | 10 kN (2250 lbf) |
下側取り付け | 0.5 in clevis (Type Dm) |
試験片厚さ | 50 mm (2 in) |
試験片幅 | 76 mm (3 in) |
試験規格 | BS 373, ASTM D 143 |
上部有効長さ | 105 mm (8.4 in) |
上側取り付け | 0.5 in clevis (Type Dm) |