Tension-Only Holders, M8 Thread
3117-025 | Tension-Only Holders, M8 Thread For 3117-020/-021 Pullrods
- M8 Thread For 3117-020/-021 Pullrods.
- Maximum Capacity 10kN at 300 deg. C.
- Maximum Capacity 10kN at 800 deg. C.
- Maximum Capacity 7kN at 850 deg. C.
- Maximum Capacity 5kN at 900 deg. C.
- Maximum Capacity 3kN at 950 deg. C.
- Maximum Capacity 2kN at 1000 deg. C.
アクセサリ直径 | 30 mm (1.18 in) |
---|---|
アクセサリ高さ | 52 mm (2 in) |
荷重容量 | 2 - 10 kN (425 - 2250 lbf) |
下側取り付け | To suit standard pullrod |
注意事項 | Force rating depends on temperature |
試験片ネジサイズ | M8 |
静的 もしくは 疲労の速度 | Static |
温度速度 | 1000°C (1832°F) |
上側取り付け | To suit standard pullrod |
+600 °C and +1000 °C Tension Only Pullrods (3117-020, 3117-021)
+600 °C and +1000 °C Tension Only Pullrods Catalog numbers 3117-020, 3117-021
- 製品
- 11/7/2005
- 132.5 KB