Compact Tension Fixtures for 25mm Thick Compact Tension Specimens
2780-119 | Compact Tension Fixtures for 25mm Thick Compact Tension Specimens
Designed in accordance with international standards such as ASTM E399, E647 & E1820Rated Capacity: ±50kN Dynamic, 100kN Static
Temperature Range: -50 to 315°C
Includes:
- Piston rod extender to reduce the minimum daylight between Loadcell and ±75mm actuator at mid-stroke to allow compact tension fixtures to touch (Quantity 1).
- Fatigue Rated Adaptors. M30 x2 right hand male to male stud with preloading wedge washers (Quantity 2)
Note: Requires 2780-120 for use with a standard 3119-600 Series Chamber
荷重容量 | ±50 dynamic, 100 static kN (±11,500 dynamic, 22,500 static lbf) |
---|---|
試験片幅 | 25 mm (0.98 in) |
試験規格 | ASTM E399, ASTM E647, ASTM E1820 |
Compact Tension Fixtures 2780 Series
Fatigue Compact Tension Fixtures for Servohydraulic machines to test crack growth. POD including 2780-118, 2780-119, 2780-120