Shoulder-End Inserts for GOST 1497 Type III Specimen #8
W-5159-B8 | Shoulder-end Inserts for GOST 1497 Type III Specimen #8
One set
Reduced section 4mm, Transition radius 1.5mm, Button diameter 9mm
Static Tensile Capacity: 25kN
Requirement: W-5159 600kN Insert holders
荷重容量 | 25 kN (5,620 lbf) |
---|---|
静的 もしくは 疲労の速度 | Static |
温度速度 | 0-38°C (32-100°F) |
Split Insert Tensile Grips W-5158 and W-5159
Instron® Split Insert Tensile Grips are designed for safe, high-volume production testing of shoulder-end or button-head machined specimens. Engineered with an operator focus, the split insert style tensile grips are easy to install, offer quick change inserts for standard specimen sizes, and promote efficient testing of a wide range of metals and alloys.