Elastomeric "O" Ring Test Fixture, Single Column Systems
2717-068 | Elastomeric "O" Ring Text Fixture
"O" Ring Test Fixture for Single Column Test Systems.
Upper fitting and lower fittings: Type Om (12 mm connection with 6 mm clevis pin). 1 kN Capacity. Requires spindle set.
For all 334X, 444X, 554X, 594X, 584X - except for model XX42s.
荷重容量 | 1 kN (220 lbf) |
---|---|
下限有効長 | 90 mm (3.5 in) |
下側取り付け | 6 mm clevis pin (Type Om) |
温度速度 | +10 to +40°C (+50 to +100°F) |
上部有効長さ | 90 mm (3.5 in) |
上側取り付け | 6 mm clevis pin (Type Om) |
2717 Series Tensions Grips
The O-ring test fixture has been designed to facilitate the testing of O-rings and similar continuous loop specimens where it is essential to minimize localized stressing in the sample.