Splitting Tensile Fixture, 6 in x 12 in Cylinder
W-1187-G | Splitting Tensile Fixture, 6 in x 12 in Cylinder
Splitting Tensile Fixture for testing 6 in x 12 in cylinders on the 400RD in accordance with ASTM C-496.
- Cylinder splitting head 14.75 in long with bearing bar surface for contact on the horizontal surface of the 12 in cylinder.
- Bearing bar surface of 2 in wide by 12 in long machined within 0.001 in of planeness with a scribed centerline.
- Bearing bar has freedom to tilt 4 degrees front to back.
- 7.125 in maximum usable vertical test opening with fixture in place.
Fixture mounts in frame with a holding stem and set screw assembly.
アクセサリ高さ | 323.9 mm (12.75 in) |
---|---|
アクセサリ長さ | 50.8 mm (2.00 in) |
アクセサリ幅 | 304.8 mm (12.00 in) |
互換性のある試験機 | 400RD |
下側取り付け | Direct |
定格圧力 | 690 MPa (100,000 psi) |
試験規格 | ASTM C496 |
上側取り付け | Ball Hitch |