ASTM F1306 specifies the test conditions for determining the characterization of flexible barrier films and laminates for slow rate penetration resistance to a driven probe at room temperature. The required calculations for this standard consist of peak force to break, energy to break, and probe penetration from initial contact to break.

The ability to characterize penetration resistance is critical for end-use performance of thin, flexible materials where a sharp object can damage the barrier’s protection. ASTM F1306 testing is common in the packaging industry, which supplies thin films to the food and consumer product sectors. Another relevant industry is battery production, which is interested in quantifying the puncture resistance of the separator films found in their Li-ion batteries.

ASTM F1306 Test SetupForce requirements of ASTM F1306 are generally lower than 250 N, making it appropriate for Instron's single column low force testing systems such as the 34SC-1 or 68SC-1, with load cells of 50 N, 100 N, or 500 N capacity. Instron's S1-14110 is a custom fixture made specifically for ASTM F1306 testing and can be ordered through our custom solutions group. 



ASTM F1306 Test Setup
1) 6800 Series Universal Testing System
2) Bluehill Universal Software
3) 2580 Series Load Cell
4) S1-14110 Custom Puncture Fixture 

 

ASTM F1306 puncture test setup
Tips and Tricks

When comparing results with other laboratories, it is important to note that the diameter of the test probe, as well as the sample test diameter, will impact load and penetration values. The ASTM F1306 standard recommends a 3.2 mm diameter hemispherical probe and a sample test diameter of 34.9 mm.

Related Content

6800 シリーズプレミアム試験機のカタログ

インストロン6800シリーズ万能試験機は、他に類のない精度と信頼性を提供します。特許申請中のオペレーター保護機能に基づき、最新のスマートクローズエアキットおよび衝突緩和機能を搭載した6800シリーズは、材料試験をかつてないほどシンプルに、スマートに、安全にします。

3400シリーズ – お手頃な試験ソリューション

引張、圧縮、曲げ、およびその他の材料特性を試験する、インストロン3400シリーズ万能試験機。

Bluehill Universalの

Bluehill Universalソフトウェアは、タッチ操作と直感的なユーザー体験のために構築されています。あらかじめ備わっている試験メソッド、すぐに試験が開始できるQuickTest、強化されたデータ出力機能、そしてサービスとの直接通信を提供する新機能Instron Connectなど、よりシンプルでスマートな試験をご体感ください。 Bluehill 2やBluehill 3などの旧バージョンソフトは、簡単に最新バージョンのBluehillにアップグレードできます。