How to Perform a Shear Test to ISO 4587

Adhesives - Determination of Tensile Lap Shear Strength of Rigid to Rigid Bonded Assemblies

Written by Meredith Bernstein

ISO 4587

 

ISO 4587 is a common testing standard used to measure the adhesive lap-shear bond strength of rigid-to-rigid assemblies. ISO 4587 is used for quality control in many industries, including aerospace, automotive, and consumer goods manufacturing. This guide is designed to introduce you to the basic elements of an ISO 4587 adhesive shear test, including an overview of the equipment, software, and samples needed. However, anyone planning to conduct ISO 4587 testing should not consider this guide an adequate substitute for reading the full standard.
What Does it Measure?

This standard is used to test the shear strength of cured bonds when adhesives are applied to materials such as metals, plastics, wood, or composites. This is a critical characteristic of any adhesive, as they can exhibit unique shear properties. Manufacturers use this test method to investigate the shear properties of bonded rigid assemblies where the force applied is parallel to the bonded area and the length of the specimen. Stress is applied to the specimens at a rate of 8.3 to 9.8 MPa per minute and the breaking load and shear strength are reported.

Materials Testing System

Testing to ISO 4587 requires a universal testing machine. System capacity will depend on the strength of the adhesive, however most tests to this standard will fall in the capacity range between 1 kN and 5 kN, appropriate for a frame such as Instron's 34SC or 68SC. If the adhesive requires a higher capacity system, Instron’s dual column table model frames are available up to 50 kN.

ISO 4587 test setup

ISO 4587 Test Setup

1. Instron 6800

2. Bluehill Universal Dashboard (2490-696)

3. 2580 Series Load Cell

4. 5 kN Pneumatic Side-Action Grips (2712-045)

 

 

 
Grips and Accessories

Pneumatic side action grips and advanced side action grips are optimal choices for testing to ISO 4587. Both types of grips are adjustable in order to offset the jaw faces and ensure that the lap joint remains centered in the grips. They both feature quick-change jaw faces that can be easily changed to accommodate different materials.

5 kN Model | 2712-045
1 kN Model | 2710-113
Helpful Tips
  •  ISO 4587 is performed on rigid specimens bonded via a lap joint, which causes the two ends of the specimen to be offset from the vertical load line of the test. It is critical that the gripping solution account for this overlap with offset jaw faces in order to ensure a true shear force application.
  • The standard requires reporting the breaking force or strength, however, it is important to remember that the shear strength is calculated by dividing the breaking force by the adhesive bond area.
Related Content

6800 シリーズプレミアム試験機のカタログ

インストロン6800シリーズ万能試験機は、他に類のない精度と信頼性を提供します。特許申請中のオペレーター保護機能に基づき、最新のスマートクローズエアキットおよび衝突緩和機能を搭載した6800シリーズは、材料試験をかつてないほどシンプルに、スマートに、安全にします。

3400シリーズ – お手頃な試験ソリューション

引張、圧縮、曲げ、およびその他の材料特性を試験する、インストロン3400シリーズ万能試験機。

Bluehill Universalの

Bluehill Universalソフトウェアは、タッチ操作と直感的なユーザー体験のために構築されています。あらかじめ備わっている試験メソッド、すぐに試験が開始できるQuickTest、強化されたデータ出力機能、そしてサービスとの直接通信を提供する新機能Instron Connectなど、よりシンプルでスマートな試験をご体感ください。 Bluehill 2やBluehill 3などの旧バージョンソフトは、簡単に最新バージョンのBluehillにアップグレードできます。

2712-04Xシリーズ空気圧式グリップ

空気圧式グリップは、広範囲の材料に対応する多用途なグリップ機能を提供します。容量は1~10 kNです。

2710シリーズ ねじ式グリップ

ねじ式グリップは、試験片をつかむための簡単かつ効果的な方法を提供し、広範囲のアプリケーションに使用できます。