ISO 527-3 Tensile Properties of Films and Sheets
Written by Dan Caesar
- Plastics
- Tension
- ISO 527-3
ISO 527-3 is an international standard used to determine the tensile properties of plastic film or sheeting. Plastic films and sheeting are a popular choice for packaging manufacturers and can be found protecting many everyday items from leftover food to consumer goods. It is critical that plastics manufacturers and packaging companies obtain an accurate mechanical profile of the plastic films they are producing to ensure that they meet the required specifications.
Material properties to be reported for ISO 527-3 include
• Tensile strength
• Yield: stress and strain
• Break: stress and strain
Film or sheeting is defined to be a plastic test specimen with a thickness less than 1 mm. Plastics with a thickness greater than 1 mm should be tested per ISO 527-2. The equivalent ASTM standard to ISO 527-3 is ASTM D882.
Recommended Testing EquipmentBecause thin film specimens break at relatively low forces, ISO 527-3 testing is often performed on a single column universal testing machine. However, due to the fact that many thin film specimens exhibit high elongation at break, an extra height single column frame or possibly a dual column frame may be required in order to test until break. Instron's 3400 and 6800 Series include a variety of test frames suitable for thin film testing, with the 6800 Series offering many advanced features for those wishing to maximize repeatability and throughput.
ISO 527-2 Test Setup
1. Instron 34SC-1
2. Bluehill Universal Dashboard (2490-696)
3.2519-1kN Load Cell
4. 1 kN Pneumatic Side-Action Grips (2712-041)
Due to the flexible, delicate nature of thin film specimens, specimen gripping can be a challenge. Pneumatic side action grips are an ideal solution because they provide an adjustable inlet air pressure to ensure that specimens can be clamped sufficiently throughout the test. When using pneumatic grips with the Smart-Close Air Kit, operators can define the inlet clamping pressure in the Bluehill Universal test method, replacing the need to manually change the pressure at the air supply’s regulator. The Smart-Close Air Kit not only promotes a safer use of pneumatic grips, but it can make testing more efficient and repeatable.
For those looking for a non-pneumatic solution for ISO 527-3 testing, Instron recommends self-tightening roller grips. Manually-tightened screw grips are not recommended for thin film testing, because the variability they add to the clamping pressure can negatively impact the repeatability of results and cause a higher frequency of improper gripping (jaw breaks or slippage).
While ISO 527-3 does not require extensometry, the use of an extensometer always results in the most accurate strain measurement. Non-contacting video extensometry is the best solution for thin film testing, as typical clip-on extensometers weigh down the specimen causing premature failure. Instron's Advanced Video Extensometer (AVE2) can measure strain as accurately as a clip-on extensometer without physically contacting the specimen.
Instron's Bluehill® Universal testing software makes it easy to report calculations in compliance with the standard. Customers who choose the Plastics method suite will receive a pre-configured test method for ISO 527-3 testing, complete with specific test parameters and calculations to help ensure compliance.
ThroughputFor labs with high-volume testing needs, several modifications to the tensile machine setup can be made to speed up the testing process and increase throughput, up to and including fully automated test systems. Fully automated systems such as Instron's AT3 are designed to incorporate specimen measurement, specimen loading, testing, and removal, and are able to run for hours without operator interaction. These systems help to reduce variability due to human error and can be left running after a shift ends to continue getting results when operators go home.
Related Content6800 シリーズプレミアム試験機のカタログ
インストロン6800シリーズ万能試験機は、他に類のない精度と信頼性を提供します。特許申請中のオペレーター保護機能に基づき、最新のスマートクローズエアキットおよび衝突緩和機能を搭載した6800シリーズは、材料試験をかつてないほどシンプルに、スマートに、安全にします。
Bluehill Universalの
Bluehill Universalソフトウェアは、タッチ操作と直感的なユーザー体験のために構築されています。あらかじめ備わっている試験メソッド、すぐに試験が開始できるQuickTest、強化されたデータ出力機能、そしてサービスとの直接通信を提供する新機能Instron Connectなど、よりシンプルでスマートな試験をご体感ください。 Bluehill 2やBluehill 3などの旧バージョンソフトは、簡単に最新バージョンのBluehillにアップグレードできます。
3400シリーズ – お手頃な試験ソリューション
引張、圧縮、曲げ、およびその他の材料特性を試験する、インストロン3400シリーズ万能試験機。
2712-04Xシリーズ空気圧式グリップ
空気圧式グリップは、広範囲の材料に対応する多用途なグリップ機能を提供します。容量は1~10 kNです。
2713-007シリーズ自己締め付けローラーグリップ
自己締め付けグリップは、主に、負荷がかかると断面積が大幅に減少するエラストマーやその他の柔軟性のある材料の精密試験のために設計されています。
AVE 2非接触式ビデオ伸び計