EN 12242「面ファスナーの引きはがし強さ」
- Textiles
- Tension
- Peel
- EN 12242
EN 12242 is a test method used to determine the peel strength of a touch and close (also known as “hook and loop”) fastener. A touch and close fastener is made up of two different types of materials: the male material is constructed with monofilament warp ends and finished to form-locking elements of either “hook” or “mushroom” shape. The female material is constructed with multifilament yarns in “loops”. When the two types of material are pressed together, the male and female elements engage to form a secure closure which can be separated by a peeling action from either end.
EN 12242 is widely used in the textile industry to evaluate different hook and loop fasteners. These fasteners have a wide range of uses, from apparel and footwear to consumer products to more industrial usage. In all cases, a complete understanding of their properties are important to ensure they perform as expected. The primary results of interest are minimum, maximum, and average peel strength.
Materials Testing SystemSystem capacity will depend on the strength of the fasteners. However, most tests to EN 12242 will fall in the 1 kN and 5 kN capacity range, making this application perfect for a single column frame such as Instron's 34SC or 68SC. Optimal gripping solutions include pneumatic side action and advanced side action grips, both of which feature quick-change jaw faces that can be easily changed to accommodate different materials as needed. Rubber-coated jaw faces are well suited to testing hook and loop fasteners.
EN 12242 Test Setup | |
---|---|
1) | 6800 Series Universal Testing System |
2) | Bluehill Universal Software |
3) | 2580 Series Load Cell |
4) | 2710 Series Advanced Side Action Grips |

For peel tests, it is critical to use a high data acquisition rate to capture all peaks and troughs to ensure all test events are fully represented in the results. Too low of a bandwidth may “dull” the results and lead to artificially low peel strength values. Instron’s 6800 series frames enable a data capture rate of up to 2.5kHz. With the Bluehill Universal Advanced Performance option, data acquisition rate can be increased to 5 kHz.
6800 シリーズプレミアム試験機のカタログ
インストロン6800シリーズ万能試験機は、他に類のない精度と信頼性を提供します。特許申請中のオペレーター保護機能に基づき、最新のスマートクローズエアキットおよび衝突緩和機能を搭載した6800シリーズは、材料試験をかつてないほどシンプルに、スマートに、安全にします。
3400シリーズ – お手頃な試験ソリューション
引張、圧縮、曲げ、およびその他の材料特性を試験する、インストロン3400シリーズ万能試験機。
Bluehill Universalの
Bluehill Universalソフトウェアは、タッチ操作と直感的なユーザー体験のために構築されています。あらかじめ備わっている試験メソッド、すぐに試験が開始できるQuickTest、強化されたデータ出力機能、そしてサービスとの直接通信を提供する新機能Instron Connectなど、よりシンプルでスマートな試験をご体感ください。 Bluehill 2やBluehill 3などの旧バージョンソフトは、簡単に最新バージョンのBluehillにアップグレードできます。
2712-04Xシリーズ空気圧式グリップ
空気圧式グリップは、広範囲の材料に対応する多用途なグリップ機能を提供します。容量は1~10 kNです。
2710シリーズ ねじ式グリップ
ねじ式グリップは、試験片をつかむための簡単かつ効果的な方法を提供し、広範囲のアプリケーションに使用できます。