ISO 11897:1999 Tear Propagation on Edge Fold of Thin Film

ISO 11897 is a test method to determine tear propagation and tear resistance properties on edge fold of sacks made from thermoplastic flexible film.

Specimens are cut in a trapezoidal shape with the edge fold position in the center.  Then, a 25mm incision is cut along the edge fold.  The specimen is pulled apart, until failure, at a constant rate of displacement. The force and displacement are recorded as the tear propagates through the entire edge fold of the specimen, and is used to calculate the resistance to tear propagation of the material.

The challenges of testing to this standard are:

  • Specimen gripping
  • Reporting calculations in compliance with the standard

Instron's Solution:

  • Specimen gripping - In order to mitigate the influence of the grips on the specimen, rubber coated faces are commonly recommended for use with either side acting manual or pneumatic grips.
  • Reporting calculations in compliance with the standard - Instron's Bluehill® Universal testing software allows users to input specimen details, set the desired test control, automatically calculate the desired results and statistics, and produce a test report all in accordance with the standard.

It is important to review ISO 11897:1999 in order to fully understand the test setup, procedure, and results requirements.

Literature

2712-04X Series Pneumatic Side-Action Grips

Pneumatic side-action grips offer a versatile gripping solution for a wide range of materials. Rated capacities between 1 and 10 kN.

  • 製品
  • 03/22/2022
  • 1.13 MB

2710 Series Screw Side Action Grips

Screw side-action grips provide a very simple and efficient method for holding test specimens in a wide range of applications. The dual – acting design of 2710-100 series grips means that jaw faces can be adjusted to accommodate different specimen thicknesses. This ensures that the line of tensile force remains concentric with the grip body. They can be equipped with a selection of interchangeable grip jaw faces in various sizes and choice of surfaces including smooth ground, rubber-coated and serrated. Line contact and special coated faces are also available.The unique ‘snap-on’ jaw face attachment makes changing faces extremely quick and simple.

  • 製品
  • 06/28/2017
  • 1.29 MB

6800 Series Premier Testing Systems Brochure

Instron 6800 Series Universal Testing Systems provide unparalleled accuracy and reliability. Built on a patent-pending Operator Protect system architecture with an all-new Smart-Close Air Kit and Collision Mitigation features, the 6800 Series makes materials testing simpler, smarter, and safer than ever before.

  • 製品
  • 02/10/2020
  • 1.93 MB

3400 Series Universal Testing Systems Brochure

Instron 3400 Series universal testing systems for tensile, compression, bend, and other material property tests.

  • 製品
  • 06/27/2022
  • 2.69 MB