ASTM F1306 Slow Rate Penetration Resistance of Flexible Barrier Films and Laminates

ASTM F1306

ASTM F1306 specifies the test conditions for determining the characterization of flexible barrier films and laminates for slow rate penetration resistance to a driven probe at room temperature. The required calculations for this standard consist of peak force to break, energy to break, and probe penetration from initial contact to break.

The ability to characterize penetration resistance is critical for end-use performance of thin, flexible materials where a sharp object can damage the barrier’s protection. ASTM F1306 testing is common in the packaging industry, which supplies thin films to the food and consumer product sectors. Another relevant industry is battery production, which is interested in quantifying the puncture resistance of the separator films found in their Li-ion batteries.

ASTM F1306 Test Setup

Force requirements of ASTM F1306 are generally lower than 250 N, making it appropriate for Instron's single column low force testing systems such as the 34SC-1 or 68SC-1, with load cells of 50 N, 100 N, or 500 N capacity. Instron's S1-14110 is a custom fixture made specifically for ASTM F1306 testing and can be ordered through our custom solutions group. 



ASTM F1306 Test Setup
1) 6800 Series Universal Testing System
2) Bluehill Universal Software
3) 2580 Series Load Cell
4) S1-14110 Custom Puncture Fixture 

 

ASTM F1306 puncture test setup

Tips and Tricks

When comparing results with other laboratories, it is important to note that the diameter of the test probe, as well as the sample test diameter, will impact load and penetration values. The ASTM F1306 standard recommends a 3.2 mm diameter hemispherical probe and a sample test diameter of 34.9 mm.

Related Content

6800 Series Premier Testing Systems Brochure

Instron 6800 Series Universal Testing Systems provide unparalleled accuracy and reliability. Built on a patent-pending Operator Protect system architecture with an all-new Smart-Close Air Kit and Collision Mitigation features, the 6800 Series makes materials testing simpler, smarter, and safer than ever before.

3400 Series - Affordable Testing Solutions

Instron 3400 Series Universal Testing Systems for Tensile, Compression, Bend, and other material property tests.

Bluehill Universal Brochure

Bluehill Universal Software is built from the ground-up for touch interaction and an intuitive user experience. Discover simpler and smarter testing with features such as pre-loaded test methods, QuickTest in seconds, enhanced data exporting: and Instron Connect – a new feature that provides a direct communication link to Service. Users of previous versions of software such as Bluehill 2 and Bluehill 3 can easily upgrade to the newest version of Bluehill.