MIL-STD-883 is a test method used in the semiconductor and microelectronics industry to determine the integrity of the connection between a semiconductor die or surface mounted passive elements to package headers or other substrates. This determination is based on the measurement of adhesion force between the die/package and the substrate, and is useful for testing microelectronic components or electronic packages such as IC chips, BGA, QFN, CSPs, and Flip Chips. MIL STD 883 is an ideal method for measuring the shear force required to to initiate failure of glue, solder, and sintered silver bonded areas.

 

Materials Testing Equipment

For die shear testing we recommend an Instron 6800 Series single or dual column system with Bluehill Universal software. 6800 Series systems are recommended due to their high crosshead displacement accuracy.




MIL STD 883 Test Setup
1) 6800 Series Universal Testing System
2) Shear tool head fixture (CP124648)
3) Microscope holder
4) 90° plate and clamp to hold specimen
5) x y theta stage to position specimen

 

MIL STD 883

Test Fixtures and Accessories

Instron Die/package shear test fixtures are designed for accurate shear force measurement in accordance with MIL STD 883 Test Method 2019. They consists of a specially designed shear tool head fixture (CP124648), a general 90-degree angle plate and clamp S4781A for shear testing specimen installation, and an x-y-theta stage (CP127130 - 5kN or S4752A - 1kN).

Using the x-y-theta stage CP127130 or S4752A, user can accurately adjust and align the position and angle of the die/package edge with respect to the edge of the shear tool. The angle plate and clamp fixture S4781A has a theta stage that can self-align the shear tool’s front face with the face of the die contact edge to ensure that the shear force is applied uniformly. The shear tool head fixture has a built-in touch sensor that enables it to precisely detect the point of contact between the shear tool and the substrate surface. This allows for accurate positioning of the shear tool above the substrate. The shear tool is interchangeable for different shear tool widths, and elevated temperature shear testing can also be performed by adding a hot stage (CP127131 or S4761A). In general, bond adhesion degrades with increased temperature, so it is essential to qualify bond strength as a function of temperature. 




MIL STD 883 Fixtures
1) Theta x-y stage
2) Shear fixture
3) Shear tool wedge

 

MIL STD 883 fixtures

Tips and Tricks

The biggest challenge in MIL STD 883 testing is to ensure that the shear head applies a uniform force distribution to an edge face of the die and to ensure that the die contact tool is perpendicular to the die mounting plane of the header or substrate. This can be even more critical when testing a die that is large or thin; as the die becomes larger and thinner, the relative size of the die-shear tool contact area against the bonding area will decrease, which can result in the stresses created by the shear tool being higher than the yield strength of the die. This will cause it to splinter or shatter before the bond is tested. Instron’s fixturing for testing to MIL STD 883 incorporates a design able to help overcome this challenge while also allowing for temperature testing. To read this standard in full, purchase MIL-STD-883.

Related Content

6800 Series Premier Testing Systems Brochure

Instron 6800 Series Universal Testing Systems provide unparalleled accuracy and reliability. Built on a patent-pending Operator Protect system architecture with an all-new Smart-Close Air Kit and Collision Mitigation features, the 6800 Series makes materials testing simpler, smarter, and safer than ever before.

Bluehill Universal Brochure

Bluehill Universal Software is built from the ground-up for touch interaction and an intuitive user experience. Discover simpler and smarter testing with features such as pre-loaded test methods, QuickTest in seconds, enhanced data exporting: and Instron Connect – a new feature that provides a direct communication link to Service. Users of previous versions of software such as Bluehill 2 and Bluehill 3 can easily upgrade to the newest version of Bluehill.