W-2005-D | Compression Platen - Spherically Seated

  • Diameter: 228 mm (9.0 in)
  • Capacity (Load): 4500 kN (1,000,000 lbf)
  • Effective Height: 127 mm (5 in)
  • Approximate Weight: 41 kgs (90 lbs)
  • Attachment: Type R1m (1.0 in) holding button