3117-036 | Tension-Only Holders, M10 Thread For 3117-030 or 3117-031 Pullrods
- M10 Optional For 3117-030 Or 3117-031 Pullrods.
- Maximum Capacity 15kN at 300 deg. C.
- Maximum Capacity 15kN at 800 deg. C.
- Maximum Capacity 10kN at 850 deg. C.
- Maximum Capacity 7.5kN at 900 deg. C.
- Maximum Capacity 5kN at 950 deg. C.
- Maximum Capacity 3kN at 1000 deg. C.