Offset Yield Strength
Offset yield strength is an arbitrary approximation of a material's elastic limit. It is the stress that corresponds to a point at the intersection of a stress-strain curve and a line which is parallel to a specified modulus of elasticity line. This parallel line is horizontally offset by a predetermined amount. The intersection point represents the yield point of the material being tested. The value of the offset (expressed as a percentage of strain) is arbitrarily defined by the material testing standard (ASTM or ISO) being used. The most common offset is 0.2%, but this can vary depending on the material. By the time the material reaches its offset yield point, it usually will have surpassed its elastic limit and experienced a small percentage of plastic strain approximately equivalent to the offset value. The testing industry has accepted this standardized approach as one method to determine the yield strength of materials that do not have an easily discernible yield point.
How is Offset Yield Strength Different from Elastic Limit?
The elastic limit is the greatest stress that can be applied to a material without causing plastic deformation. The offset yield point differs from the elastic limit, as offset yield will generally occur beyond the material's elastic limit.
How is Offset Yield Strength Different from Proportional Limit?
The proportional limit is the point on a stress-strain curve where the linear, elastic deformation region transitions into a non-linear, plastic deformation region. Offset yield strength differs from the proportional limit as offset yield can be beyond a material's linear region.
Série 3400 - Soluções acessíveis para testes
Sistemas universais de teste Instron da série 3400 para testes de tração, compressão, flexão e outros testes de propriedade de material.
Fale conosco
Fale conosco e saiba mais sobre nossas soluções para o setor e de testes. Nossas equipes de atendimento ao cliente estão à disposição e prontas para ajudar.