ASTM E290 Bend Testing of Material for Ductility
- Metals
- Flexure
- ASTM E290
ASTM E290 describes the testing requirements used to determine the ductility of metals through bend testing. Bend testing helps provide a visual indication of the material's ductility. ASTM E290 is divided into four methods for bending the specimen:
- Guided Bend
- Semi-Guided Bend
- Free-Bend
- Bend and Flatten.
These tests are performed by supporting the two ends of a specimen while loading it at the center with a mandrel or plunger. The test is completed when the designated angle of the bend, or other specified condition, has been reached. Afterwards, the specimen is visually inspected for cracks or defects, and failure is determined by the size of the cracks and imperfections allowed by the material specification.
Materials Testing SystemFor ASTM E290 testing we recommend using an Industrial Series DX or HDX model with Bluehill Universal software and a W-6810 test fixture. This fixture allows for adjustment of the support span and is supplied with various sizes of loading mandrels to accommodate different specimen thicknesses. The loading supports are held together with two tie rods to provide extra stiffness during loading. The DX or HDX Model dual test space load frames allow the bend test fixture to be positioned in the lower compression test space. Any tensile testing can also be accomplished in the upper tensile test space.
ASTM E290 Test Setup | |
---|---|
1) | Instron 1000 HDX |
2) | W-5340 Hydraulic Wedge Action Grips |
3) | W-6810 test fixture |

High Force Universal Testing Machines Brochure
Instron's high force systems include electromechanical and high-capacity hydraulic testing systems for tension and compression applications. Force capacities range from 100 kN to 2000kN.
Industrial Series HDX Models
Featuring a dual test space and long test stroke, these hydraulic frames are available in 1,000 kN (225,000 lbf) and 1,500 kN (337,500 lbf) capacities.
Bluehill Universal Brochure
Bluehill Universal Software is built from the ground-up for touch interaction and an intuitive user experience. Discover simpler and smarter testing with features such as pre-loaded test methods, QuickTest in seconds, enhanced data exporting: and Instron Connect – a new feature that provides a direct communication link to Service. Users of previous versions of software such as Bluehill 2 and Bluehill 3 can easily upgrade to the newest version of Bluehill.