Stress Control and Yielding Material

Since the first materials testing machines were used for tensile testing of metals, one option of performing the test has been to control the rate at which you apply load to the specimen, or apply stress.

Posted By David Fry

 Sep 25, 2013

blog

Upper Yield Calculations—Discontinuous Yielding/YPE Material

Following a recent lab visit, I thought it was worth writing a quick post to share an example of how labs sometimes incorrectly calculate yield strength. While visiting a testing lab for unrelated issues, my colleagues and I were discussing how the customer runs both continuous and discontinuous material with the same method (Non-YPE and YPE). For historical reasons, they have updated their Series IX methods to Bluehill 3 with little knowledge of why, when or by whom the methods were setup.