D790-02 Standard Test Methods for Flexural Properties of Unreinforced and Reinforced Plastics and Electrical Insulating Materials
D6272-02 Standard Test Method for Flexural Properties of Unreinforced and Reinforced Plastics and Electrical Insulating Materials by Four-Point Bending
C393-00 Standard Test Method for Flexural Properties of Sandwich Constructions
C78-02 Standard Test Method for Flexural Strength of Concrete (Using Simple Beam with Third-Point Loading)
C293-02 Standard Test Method for Flexural Strength of Concrete (Using Simple Beam With Center-Point Loading)
C1161-02b Standard Test Method for Flexural Strength of Advanced Ceramics at Ambient Temperature
D143-94(2000)e1 Standard Test Methods for Small Clear Specimens of Timber
D6109-97e1 Standard Test Methods for Flexural Properties of Unreinforced and Reinforced Plastic Lumber
D198-99 Standard Test Methods of Static Tests of Lumber in Structural Sizes
C1341-00 Standard Test Method for Flexural Properties of Continuous Fiber-Reinforced Advanced Ceramic Composites
D5572-95(1999) Standard Specification for Adhesives Used for Finger Joints in Nonstructural Lumber Products
ISO
178:2001 Plastics-Determination of Flexural Properties